dangerous amateur
Hazard to Others
 
Posts: 144
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
ETN recrystallization for max density
I did that before, but never bothered obout crystal shape and density.
My ETN is usually extremely fluffy.
When using hot ethanol it gets needle shaped.
However, both are a pita to handle, esspecialy when trying to fill it in small tubes.
How does your technique look like, and what solvent do you prefer (I've got methanol too)?
Will the density suffer if one is growing large crystals (that will be likely crushed when pressing??)?
|
|
|
Ral123
International Hazard
   
Posts: 735
Registered: 31-12-2011
Member Is Offline
Mood: No Mood
|
|
Density is not a problem at all with ETN. You add NG and it's maximum density. But then you need good detonator/booster. I'd stay with the needle
crystals for small things and base charges.
|
|
|
Fuse
Harmless
Posts: 16
Registered: 25-2-2013
Member Is Offline
Mood: No Mood
|
|
In the recrystallization process via hot ethanol i've tryed two ways to obtain high density:
1) Ethanol evaporate and you get ETN needles
2) Adding water to the Ethanol/ETN very slowly and mixing continuously the solution (no needle formation).
|
|
|
DrManhattan
Harmless
Posts: 32
Registered: 24-1-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Ral123  | | Density is not a problem at all with ETN. You add NG and it's maximum density. But then you need good detonator/booster. I'd stay with the needle
crystals for small things and base charges. |
What is the sensitivity and storage stability of such a composition? Considering that etn and ng are sensitive to even the smallest of caps i would be
surprised if it required a booster.
|
|
|
XeonTheMGPony
International Hazard
   
Posts: 1601
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
Well if made care fully and well purified with a bit of urea as a acid scavenger it lasts a very long time. I have some stored for a year in perfect
shape.
|
|
|
Rocinante
Hazard to Others
 
Posts: 121
Registered: 13-11-2017
Member Is Offline
Mood: No Mood
|
|
Maximum density esters can suffer low VOD without a small booster, esp. regarding NC/EGDN. However, this is unlikely to be a problem in ETN/NG.
|
|
|