Author: Subject: Gold Oxide
Tdep
International Hazard
*****




Posts: 504
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: *PhD Crisis Time*

[*] posted on 6-4-2013 at 05:51
Gold Oxide


Hey, I have a tiny amount of gold (mainly scrap gold) and I want to turn it into gold oxide.

My first thought was to put it into solution with KNO3+HCl and then add sodium hydroxide/carbonate to precipitate gold hydroxide/carbonate which I could then decompose into gold oxide.

But is it that simple or does the chloroauric acid complex not behave as straightforward as I hoped?
View user's profile View All Posts By User
Motherload
Hazard to Others
***




Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline

Mood: Shitty

[*] posted on 6-4-2013 at 18:27


And that would be energetic how ?
Also ... Aurous or Auric ?
Neutralization of Chloroauric acid with a alkali carbonate should form the hydrated Auric oxide..
Using carbonate will minimize the chance of forming complexes.

[Edited on 7-4-2013 by Motherload]




"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
View user's profile View All Posts By User
Tdep
International Hazard
*****




Posts: 504
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: *PhD Crisis Time*

[*] posted on 7-4-2013 at 00:48


Auric yeah. So adding a carbonate to chloroauric acid will create gold oxide, no gold carbonate formed?

Energetic?
View user's profile View All Posts By User
weiming1998
International Hazard
*****




Posts: 616
Registered: 13-1-2012
Location: Western Australia
Member Is Offline

Mood: Amphoteric

[*] posted on 7-4-2013 at 01:41


Quote: Originally posted by Tdep  
Auric yeah. So adding a carbonate to chloroauric acid will create gold oxide, no gold carbonate formed?

Energetic?


By itself, hydrated gold oxide is most probably not energetic (although it decomposes to oxygen and gold easily when heated). It can probably be used to make energetic thermite mixtures with aluminium or magnesium, but it's not worth it. Better to use it, or finely-powdered gold, for non-energetic purposes (e.g, as a catalyst for certain reactions)

[Edited on 7-4-2013 by weiming1998]
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 7-4-2013 at 03:16


Fulminating gold?
View user's profile View All Posts By User
Motherload
Hazard to Others
***




Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline

Mood: Shitty

[*] posted on 7-4-2013 at 10:48


How much gold do you have and of what purity ?
I thought about fulminating gold but it hardly seems worth it.




"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
View user's profile View All Posts By User
aspiresquarelinks
Unregistered




Posts: N/A
Registered: N/A
Member Is Offline


[*] posted on 8-4-2013 at 02:09


Gold Oxide is a highly insoluble thermally stable Gold source suitable for glass, optic and ceramic applications. Two independent pathways for corrosion of elements are hydrolysis and oxidation by oxygen. The combination of water and oxygen is even more corrosive.



Tdep
International Hazard
*****




Posts: 504
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: *PhD Crisis Time*

[*] posted on 8-4-2013 at 03:27


Well I was thinking about doing a gold thermite. That should be pretty energetic :D
Or is it really not worth the effort?
View user's profile View All Posts By User
Finnnicus
National Hazard
****




Posts: 342
Registered: 22-3-2013
Member Is Offline


[*] posted on 8-4-2013 at 04:24


You gold potentially lose like 30-50$ of gold.



View user's profile View All Posts By User
gregxy
National Hazard
****




Posts: 421
Registered: 26-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 8-4-2013 at 11:02


Gold thermite???


I don't think you will get much bang for your buck.


(sorry, I couldn't resist).
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 8-4-2013 at 11:16


Not worth it, in both the monetary and empirical sense. Gold thermite will look like every other thermite, and if the thermite was big enough, there might be some molten gold in your crucible afterwards.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Tdep
International Hazard
*****




Posts: 504
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: *PhD Crisis Time*

[*] posted on 8-4-2013 at 20:55


Quote: Originally posted by gregxy  


I don't think you will get much bang for your buck.



Aww maybe not then, that pun has disheartened me quite a bit haha. Thought it would be the most viloent thermite, becuase of gold's low reactivity?

[Edited on 9-4-2013 by Tdep]
View user's profile View All Posts By User
Motherload
Hazard to Others
***




Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline

Mood: Shitty

[*] posted on 9-4-2013 at 06:17


It maybe violent .... But you can similar results with lot less with CuO thermite or flash powder.



"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
View user's profile View All Posts By User
Tdep
International Hazard
*****




Posts: 504
Registered: 31-1-2013
Location: Laser broken since Feb 2020 lol
Member Is Offline

Mood: *PhD Crisis Time*

[*] posted on 9-4-2013 at 06:24


Of course but.... gold.. thermite... ah fine. I give up.

But the fulminating gold looks fascinating! There a thread for this already?
View user's profile View All Posts By User
Motherload
Hazard to Others
***




Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline

Mood: Shitty

[*] posted on 10-4-2013 at 08:19


Ok ok ... You want to try Gold thermite. Lets try 2 experiments in one ....
How about you also cover a small quantity with a a small beaker or similar .... To see if gold vapor will deposit itself on the glass. Quartz/Gold mirrors are more efficient in reflecting infra red than standard mirrors.
Also this way you might some of your gold back..




"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
View user's profile View All Posts By User