Author: Subject: Chlorothermal reactions (chloride thermites) for preparing AlCl3 and KAlCl4
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2014 at 04:50


deltaH: I doubt that passivation is the problem here. My Ti dissolves easily in hot, concentrated H2SO4 and hot, 37 w% HCl. I don't really see what a bit of Al would do but I might try it. Sure, Al does reduce TiO2 very slowly.

There is of course already a lab bench preparation of TiCl4: TiO2 + NaCl + potassium persulphate (see 'plante').

I think I'll test my AlCl3 as a Friedel Crafts catalysts, need to get some 'bits' together for that. I will also try and scale this up a bit with a more suitable apparatus.




View user's profile Visit user's homepage View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 20-4-2014 at 06:07


Thanks blogfast for indulging me.

To elaborate my thinking: since ZnCl2 behaves as a mild HCl of sorts by my analogy, it is insufficiently strong an etchant to dissolve the passivisation layer of titanium in the same way titanium does not react with dilute HCl. The purpose of adding some Al is twofold, as a reducing agent and also the anhydrous AlCl3 generated, being a strong lewis acid, could help dissolve the passivation layer.

Since the thermo's say this should work, I'm inclined to think that something is preventing it from starting... hence I turn to the usual suspect in such cases.



[Edited on 20-4-2014 by deltaH]




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2014 at 08:28


Quote: Originally posted by deltaH  

Since the thermo's say this should work, I'm inclined to think that something is preventing it from starting... hence I turn to the usual suspect in such cases.

[Edited on 20-4-2014 by deltaH]


The thermos say nothing about kinetics, of course. Maybe it's just dead slow or needs a catalyst of sorts.

On the plus side, if you need something that resists boiling ZnCl2, look no further ;)




View user's profile Visit user's homepage View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 4-5-2014 at 05:09


I ran another AlCl3 preparation, this time with a simple and effective geometry:



A large borosilicate boiling tube (OD about 25 mm, length 145 mm) is horizontally clamped up, in such a way that its neck penetrates into a 250 ml Simax wide necked reagent bottle, which will act as a condenser flask.

A freezer bag containing some ice and a bit of water is then draped over the reagent bottle, the reagent mix loaded and ignited.

The AlCl3 vapours collect in the condenser flask and condense (despite the rather large gap, with minimal losses). The flow of AlCl3 can be regulated somewhat by adding gentle heat from a medium hot Bunsen burner or by withdrawing it.

I would recommend using a similar set up to anyone preparing AlCl3 (using whatever chlorinating agent) because the risk of blockage by solid condensed AlCl3 is basically zero.

[Edited on 4-5-2014 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 4-5-2014 at 06:31


Ah, very simple procedure! I like it. This way one can just keep the condensed AlCl3 in the reagent bottle - Although it's much bigger than needed. Or perhaps the reaction could be done many times without emptying the bottle, until it's full, and can be stored as is.
Either way, this is about as easy as it gets to make anhydrous aluminum (III) chloride. No chlorine, no gas generators, no tubes or SS pipes, condensing is so easy.




View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 4-5-2014 at 07:24


Quote: Originally posted by Zyklonb  
No chlorine, no gas generators, no tubes or SS pipes, condensing is so easy.


Zb:

I'd still like to try the chlorination with HCl with this set up. But I'd refrain from chlorine, if I was you. The HCl reaction, according to Holleman ('Inorganic Chemistry'), is self-sustaining once initiated. The Cl2 reaction will by definition be much more exothermic, thus harder to control I think.

Brauer (Preparative Inorganic Chemistry, see library) gives a prep for Al + HCl but not for Al + Cl2, for instance...

[Edited on 4-5-2014 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 4-5-2014 at 09:58


Excellent work blogfast, I'm happy you got it to work!



Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 4-5-2014 at 11:28


Quote: Originally posted by deltaH  
Excellent work blogfast, I'm happy you got it to work!


Thanks. Can't believe I was so stupid to try this first with fairly narrow tubes and not expect blockages. That would only have been possible by keeping them at 190 C or so. Hindsight is 20/20, I suppose...

I need to add that this set up can also be used to re-sublime the AlCl3, for instance to remove any ZnCl2 impurity that may have come over too.

[Edited on 5-5-2014 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 19-2-2016 at 12:02


Chemplayer made a video of this reaction :cool:

https://www.youtube.com/watch?v=g7sS69fQMsk

Yields are crap though, weird.

[Edited on 19-2-2016 by deltaH]




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 19-2-2016 at 12:12


Quote: Originally posted by deltaH  
Chemplayer made a video of this reaction :cool:

https://www.youtube.com/watch?v=g7sS69fQMsk

Yields are crap though, weird.


I know.

Yields could be improved fairly easily, IMHO. It's a solid-solid reaction, that explains low yields, I think.

[Edited on 19-2-2016 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 20-2-2016 at 01:29


Zinc chloride and aluminum definitely do react to produce aluminum chloride, but capturing the product is tricky. I have tried copper (II) chloride/aluminum thermite, and it definitely produces AlCl3, but it is tricky to control the rate of the reaction. It may be possible to run it in ethyl acetate (or not, and that might be dangerous... not sure). I am getting a 125 cm quartz tube in a few days and plan to try out the classic method with anhydrous HCl. I think by heating one end of the tube with nichrome wire and cooling the other with copper tubing, I should be able to convert aluminum to AlCl3 almost quantitatively.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2016 at 07:24


Quote: Originally posted by JJay  
Zinc chloride and aluminum definitely do react to produce aluminum chloride, but capturing the product is tricky. I have tried copper (II) chloride/aluminum thermite, and it definitely produces AlCl3, but it is tricky to control the rate of the reaction. It may be possible to run it in ethyl acetate (or not, and that might be dangerous... not sure). I am getting a 125 cm quartz tube in a few days and plan to try out the classic method with anhydrous HCl. I think by heating one end of the tube with nichrome wire and cooling the other with copper tubing, I should be able to convert aluminum to AlCl3 almost quantitatively.


Ethyl acetate won't work, I think. It's BP is only 77 C. The solid-solid reaction needs strong heating to initiate and the reaction front exceeds 180 C (otherwise the AlCl3 could not sublime off). Ethyl acetate is an aprotic solvent.

For Al + anh. HCl look in the library's Georg Brauer 'Hbk. of Preparative Inorganic Chemistry', it has a procedure + apparatus. Done correctly it will be near-quantitative.

[Edited on 20-2-2016 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 20-2-2016 at 07:42


Right, but in water, the reaction proceeds at room temperature.

IIRC, Brauer suggested using a "parting flask" at temperatures that looked dangerous for borosilicate glass.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2016 at 08:22


Quote: Originally posted by JJay  
Right, but in water, the reaction proceeds at room temperature.



Water is a very 'special' solvent, though. If the ZnCl2 fully dissociates in ethyl acetate, as it does in water, then the reaction may be viable. Otherwise you'll have ZnCl2 particles sloshing against Al particles and no party.

Re. Al + anh. HCl, acc. my old A.F. Holleman ('Inorganic Chemistry'), after initially heating the Al, once the reaction starts it is self-sustaining. That sounds plausible, as for:

Al(s) + 3 HCl(g) ===> AlCl3(g) + 3/2 H2(g)

... I estimate an Enthalpy of Reaction of about - 390 kJ/mol of AlCl3(g) (adjusted for the vapourisation Enthalpy of AlCl3(g)). Compare it with the ZnCl2/Al reaction: only about - 75 kJ/mol.

So, quite a lot of heat!


[Edited on 20-2-2016 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 20-2-2016 at 16:28


Oh for zinc chloride and aluminum? I just got some media bottles and a thermometerless distillation adapter in the mail today.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2016 at 18:31


Quote: Originally posted by JJay  
Oh for zinc chloride and aluminum? I just got some media bottles and a thermometerless distillation adapter in the mail today.


ChemPlayer's version was basically a simple distillation apparatus. Call it a 'dry distillation'.