Getting chromium compounds out of chromated metal?
Some time ago I tried the classic HCl+H2O2+[chromated-zincated-otherated steel] and got a vigorous reaction with the release of
perchloric acid and other stuff, like chromic anhydride.
Now, is there a way to isolate any chromium compound out of that?
Is there any other way to remove chromium from a chromated metal piece?
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by valeg96 | [...] and got a vigorous reaction with the release of perchloric acid and other stuff, like chromic anhydride.
|
Perchloric acid as in HClO<sub>4</sub>? That strikes me as impossible.
'Chromic anhydride': as in CrO<sub>3</sub>? Again, unlikely to form in an aqueous solution. What's more, in acid conditions Cr(VI) is
reduced by H<sub>2</sub>O<sub>2</sub> to Cr(III).
If recovering chromium from scrap metal is your goal, scrap stainless steel is a better feed stock, IMO. It contains a minimum of 10.5 w% of Cr
(Wiki).
[Edited on 27-4-2014 by blogfast25]
|
|
LanthanumK
Hazard to Others
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Chromated metal is only coated, so an insignificant amount of chromium is present.
hibernating...
|
|
HgDinis25
Hazard to Others
Posts: 439
Registered: 14-3-2014
Location: Portugal
Member Is Offline
Mood: Who drank my mercury?
|
|
What do you mean by releasing? Did you worked your products all the way to Chromic Anhydride, for instance, or are you saing that they formed by the
reaction between the steel and the HCl/H2O2?
AFAIK, it's impossible to produce CrO3 or even perchloric acid, in the conditions mentioned.
|
|