[*] posted on 1-7-2014 at 20:08


So, I just made Thulium Chloride, Bromide, and Nitrate solutions. I have now used up about half of my Tm sample.

This time, I was much more careful to use only slightly excess acid (HCl, HBr, and HNO3). Because of this, the reactions are proceeding much more slowly and are not complete yet - each test tube still has a tiny piece of Tm at the bottom with a trail of bubbles rising from it.

However, I can definitely tell that the TmCl3 and Tm(NO3)3 solutions are very pale green. The TmBr3 is more ambiguous.

Maybe the problem with the H2SO4 was way too much acid. Still - you would think that the crystals I would get at the end would be Tm2(SO4)3 still.
View user's profile View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 1-7-2014 at 20:10


IrC - thanks for the photos - I would say that the comparison to my sample is unclear, but that is probably due to your sample being formed by a different process, resulting in a different surface appearance.
View user's profile View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 1-7-2014 at 21:00


Quote: Originally posted by sbreheny  
IrC - thanks for the photos - I would say that the comparison to my sample is unclear, but that is probably due to your sample being formed by a different process, resulting in a different surface appearance.


More likely due to mine sitting in a plastic envelope for 10 years in a hot storage room. The grain structure is what you should be closely comparing. More important than minor color differences from various levels of surface oxidation over years. Your sample may be closer to it's date of creation and stored better.




"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 168
Registered: 5-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 2-7-2014 at 04:33


Quote: Originally posted by sbreheny  
you would think that the crystals I would get at the end would be Tm2(SO4)3 still.

No, but a hydrate. Probably the octahydrate. Your photo shows rather a crystal mass and not well formed crystals. Thulium sulfate often forms a supersaturated solution and crystallizes out very fast after a while. It's not so easy to get well formed crystals.

Here is a comparison of Tm(III) in water and in ca. 25 % HCl. There is only a very little difference. But this difference is not easy to identify with the naked eye. I would still call it "very pale green":
3.jpg - 59kB
left: water, right: HCl

1.jpg - 49kB
The solid and "neutral" TmCl3 * x H2O - pale green like the sulfate

If the chloride is heated with sulfuric acid and further heated until white fumes of sulfuric acid appear, white crystals form. They don't look the slightest bit green. This is probably the stuff which you got in your first try. Thulium sulfate with less than 8 moles water per mole:
2.jpg - 89kB

Quote: Originally posted by Brain&Force  
Terbium does form a hexaaquadichloro complex (which is highly triboluminescent).

Do you have a source for this claim? Which complex do you mean?




My youtube channel: Joe Black
View user's profile Visit user's homepage View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 2-7-2014 at 08:50


http://www.researchgate.net/publication/231348013_Crystal_st...

I don't have access, but this paper references a complex, hexaaquadichloroterbium(III) chloride, which appears to be highly triboluminescent.

Those are interesting results Pok, but they don't seem to explain the black stuff in sbreheny's crystals. I'm guessing any complexation that's occurring due to the presence of the chloride ion is minimal.




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 168
Registered: 5-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 2-7-2014 at 10:11


Quote: Originally posted by Brain&Force  
hexaaquadichloroterbium(III) chloride


= 6 H2O + 2 Cl + Tb + Cl
= TbCl3 * 6 H2O

This is ordinary terbium chloride (hexahydrate). The complicated name is just a more precise description of the structure of the molecule. The article says that it's triboluminescence (TL) wasn't observed until 1989. Therefore, it's very improbable that the TL is bright. The article doesn't specify the brightness of terbium trichloride hexahydrate (not even "bright" or so). This info should be specified in the literature elsewhere. But I think it is very very weak and not comparable to the other 2 named in the paper. I think the authors are a bit imprecise when talking about "3 brilliant triboluminescent complexes". They also call it "terbium hexahydrate" in one passage which is absolute nonsense.

But yes. Here we see that nearly every hydrated salt is a complex in the solid state, also the lanthanide chloride hexahydrates. This can explain the difference of the colour of hydrated vs. water-free thulium sulfate. IrC cited a wikipedia article which claims that. Although the "reference" is a simple web page, it sounds reasonable.




My youtube channel: Joe Black
View user's profile Visit user's homepage View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 2-7-2014 at 13:38


Hmm...I knew that most salts were solid state complexes. It's good to know that terbium chloride isn't as triboluminescent as the paper states. I guess these people didn't bother to revise their paper...

I've heard that neodymium can form acid and basic sulfates, so that may be possible with thulium as well. But the loss of water is the more likely cause, as water molecules do most of the coordinating and produce the colors we see in transition metal salts, and the same is seen with many dehydrated sulfates (like copper sulfate, for example).




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 4-7-2014 at 09:51


sbreheny, I'm curious, is your thulium salt magnetic? I have some terbium sulfate which is definitely paramagnetic.



At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
Pok
potassium Prometheus
***




Posts: 168
Registered: 5-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 4-7-2014 at 12:25


My Tm oxide and sulfate are magnetic (using a very strong magnet). Also the oxides of: Er, Ho, Eu (weak)

Not the oxides of: Pr, Nd, Y, Sm, Yb, Sc, Lu




My youtube channel: Joe Black
View user's profile Visit user's homepage View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 6-7-2014 at 21:12


Yes, the salt (presumably Thulium Sulfate) is slightly attracted to a magnet. It is not strong enough to be affected through the wall of a glass bottle but if I lower the NdFeB magnet down on top of it, at about 1mm away the powder jumps to the magnet and sticks to it.

Now, I have some interesting results to show. I tried the thiocyanate test and I need some help interpreting it. I have five test tubes. The first one (on the left) had a sample of Tm added. The next one had 1mL of my technical grade H2SO4 added. Next one had 1mL of ACS reagent grade H2SO4 added. The next one had a tiny amount of iron powder added, and the last one had only distilled water added.

For the iron one, I actually put in 100mg of iron powder and dissolved it in 2mL water and 1mL 70% HNO3 (note to self once again - this produced a nice little cloud of NO2 which I had to avoid - I really do need to get a hood!). I then poured out most of the resulting solution and diluted it about 10:1 with distilled water.

Anyway, I then added to each one (except the iron) 1mL of 70% HNO3, my idea being that it would convert any iron into Fe3+ ions. I then added 3mL more distilled water to each and finally approximately 250mg of KSCN.

At first, this happened:
Start

Then, after about 20 seconds, it looked like this:
Settled

I tried agitating the two H2SO4 samples to re-mix the red and clear layers, but then they released a small amount of NO2 and the solution became a very pale blue:
Almost Final

Finally, even the Tm sample underwent the same change (released a small amount of NO2 and turned light blue). The distilled water sample remained light pink and the Fe remained dark blood red.
Final

Now, of course, the Fe behaved as expected. The fact that the distilled water showed some iron could be real or it could be due to some accidental cross-contamination when I was using a dropper to add to each test tube in succession. However, I really do not understand what happened with the first three. Any ideas?

Thanks,

Sean
View user's profile View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 6-7-2014 at 21:15


Another interesting data point - I purchased a 1g sample of Tm from Metallium. When I compare this to my previous sample, the appearance is similar BUT I cannot get the Tm from Metallium to show visible attraction to a magnet whereas the earlier sample does show very slight attraction. I suspect that there is some iron contamination in my original Tm. Note that the Tm sample I used in the thiocyanate test was the earlier one (from RareEarthMetalsLLC).
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 6-7-2014 at 21:50


If you look at the magnetism video that I posted, you'll see thulium is attracted to a neodymium magnet. What kind of magnet are you using? Thulium should be slightly paramagnetic.



At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 7-7-2014 at 00:54


Quote: Originally posted by sbreheny  
Another interesting data point - I purchased a 1g sample of Tm from Metallium. When I compare this to my previous sample, the appearance is similar BUT I cannot get the Tm from Metallium to show visible attraction to a magnet whereas the earlier sample does show very slight attraction. I suspect that there is some iron contamination in my original Tm. Note that the Tm sample I used in the thiocyanate test was the earlier one (from RareEarthMetalsLLC).


I ran into similar troubles buying different rare earths in 20 to 150 gm amounts from various ebay sellers. In my case of using the elements for doping glow powders even microscopic Fe impurities caused large problems. I surmised this was caused by so many sellers using hacksaw blades (or motorized saws) to cut the pieces from a larger one. Of course this was after making the same mistake myself in my first year conducting glow powder experiments and learning the hard way never cut rare earths with metal tools if purity is important.

Also, have you tried putting them on styrofoam floating in water as I have seen done in a few videos on the subject? He was able to observe even tiny effects in this way. Here is a link to the first of 3 videos he did on this subject.

http://www.youtube.com/watch?annotation_id=annotation_828992...




"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 7-7-2014 at 04:56


sbreheny:

Re. your thiocyanate tests.

Firstly, check all reagents used for iron.

Secondly, use hydrogen peroxide (check it too for iron) instead of nitric acid. With the latter the oxidation is often delayed somewhat (my experience also with Fe(II)), not to mention the NO2 fumes that stink. Heat the tubes to destroy any excess H2O2, then cool and add thiocyanate.


[Edited on 7-7-2014 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 7-7-2014 at 13:14


Thanks for the advice, I will try that. However, do you have any possible explanation of why the first three tubes would turn red initially but then become clear? Do you think that the red color was not the Fe-Thiocyanate complex but rather NO2 and as the solution cooled, it released the NO2?
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 7-7-2014 at 13:22


I've had that occur sometimes with extremely small amounts of ferric ion and extremely large amounts of thiocyanate. The same thing occurs with small amounts of starch and large amounts of triiodide. Not sure what causes this but it's likely an equilibrium thing.

It's sad to see your distilled water contains iron. Try deionized water, if available.

[Edited on 7.7.2014 by Brain&Force]




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 7-7-2014 at 16:31


I am using an NdFeB magnet which is N35 or N42 (I don't know why the package does not say for sure which it is but that is the range). I just tried it again and I see that the difference I observed was just due to the shape of the bottom of the bottles the two samples are in. The older sample is in a smooth-bottom bottle. The newer one (Metallium) is in a concave-shaped bottom bottle. When I put the magnet directly near the samples, both are weakly attracted to the magnet. If I put the new sample in the old one's container, I can indeed slide it around the bottom by applying the magnet from the outside.

Quote: Originally posted by Brain&Force  
If you look at the magnetism video that I posted, you'll see thulium is attracted to a neodymium magnet. What kind of magnet are you using? Thulium should be slightly paramagnetic.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 8-7-2014 at 04:35


Quote: Originally posted by sbreheny  
However, do you have any possible explanation of why the first three tubes would turn red initially but then become clear?


My own guess is destruction of the thiocyanate by the nitric acid.

With peroxide, try using sparing, reasonable amounts (calculate, if you can).

A little known fact is that when you add nitric to Fe(II) initially the solution darkens due to formation of an Fe(NO)<sup>2+</sup> complex. This can create the illusion that the oxidation (Fe II == > Fe III) is over, when it isn't.




View user's profile Visit user's homepage View All Posts By User
kmno4
International Hazard
*****




Posts: 1439
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 8-7-2014 at 15:14


Fe/SCN test for small (expected) amounts of Fe must be done in strongly acidic conditions, 1 M total concentration of HCl would be ok. High (relatively) amount of thiocyanate should be used (because of not very large stability of Fe(III) complex).
And the most important: extraction of formed red complex into polar organic phase. Extracted complex (in form of "ferrithiocyanate acid") is more stable in this medium than in water.
For testing in tubes, 0,5 cm3 (or similar amount) of organic solvent should be used, with shaking and allowing to separate.
Good extractants are higher alcohols, for example (n-)butanol (interesting, n-butyl acetate does not extract this complex from water)
PS. instead of 1 ml 70% HNO3, one or two drops would be better, but I prefer H2O2 instead of HNO3.




Слава Україні !
Героям слава !
View user's profile View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 8-7-2014 at 18:16


Hmmm. OK, so I have one recommendation to use H2O2 and another one to use H2SO4 and then separate the red complex using a polar organic solvent. I don't really need the result to be stable, just as long as it persists long enough for me to see it and I can be sure that I didn't screw up the test and do something wrong (I was not expecting the color to disappear so I assumed I did something wrong and perhaps the initial color change was not indicative of iron).

If I use H2SO4, won't I have Fe(II) ions instead of Fe(III)? Will they still react with the SCN to form the red complex?

As for using Butanol to separate out the red complex from water - the wiki article on Butanol says that it is fairly soluble in water, so I don't understand why it would form a distinct layer.

Sean

Quote: Originally posted by kmno4  
Fe/SCN test for small (expected) amounts of Fe must be done in strongly acidic conditions, 1 M total concentration of HCl would be ok. High (relatively) amount of thiocyanate should be used (because of not very large stability of Fe(III) complex).
And the most important: extraction of formed red complex into polar organic phase. Extracted complex (in form of "ferrithiocyanate acid") is more stable in this medium than in water.
For testing in tubes, 0,5 cm3 (or similar amount) of organic solvent should be used, with shaking and allowing to separate.
Good extractants are higher alcohols, for example (n-)butanol (interesting, n-butyl acetate does not extract this complex from water)
PS. instead of 1 ml 70% HNO3, one or two drops would be better, but I prefer H2O2 instead of HNO3.
View user's profile View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 9-7-2014 at 04:32


Quote: Originally posted by sbreheny  
If I use H2SO4, won't I have Fe(II) ions instead of Fe(III)? Will they still react with the SCN to form the red complex?



Both HCl and H2SO4 are non-oxidising acids (in this context) and rely on the oxidative power of H<sub>3</sub>O<sup>+</sup>. This ion can oxidise iron only to the ferrous form, so both HCl and H2SO4 lead to Fe<sup>2+</sup>, which does NOT form the blood red coloured complex with thiocyanate.

That is why an oxidiser like H2O2 needs to be used prior to adding the thiocyanate, so that the peroxide oxidises all ferrous promptly to ferric iron, which does yield the coloured complex.

I've never heard of extracting the complex with organic solvents. It may present some improvement but in my experience simple testing for Fe<sup>3+</sup> does not require this extra complication.

In strongly oxidising conditions the thiocyanate ions probably won't last very long but as you pointed out it is sufficient to see the complex for a brief but definite time to confirm the presence of iron.

As kmno4 suggested, keep the amount of oxisiser low: there really isn't that much iron in a couple of ml of your solutions. And you don't even need to oxidise ALL iron to Fe (III) to actually get a positive result, even a partial oxidation will give a positive if Fe is present at all.

Re. n-butanol, with 73 g/L water solubility (Wiki) a two phase system will form if you use more than 73 g of n-butanol per L of water. 1 ml n-butanol per ml of solution would definitely do it. But this is more useful if one wanted to actually isolate the complex than for a simple test, IMHO.


[Edited on 9-7-2014 by blogfast25]




View user's profile Visit user's homepage View All Posts By User
Pok
potassium Prometheus
***




Posts: 168
Registered: 5-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 9-7-2014 at 08:00


I don't see a reason for you to test for iron. Thulium is very slightly magnetic as your sample is. This cannot be explained by the very low iron content! Even if it is contaminated with iron, it is very very low as you can see from your test. This low contamination won't lead to such a rather strong attraction to a magnet!

Your 100 mg of iron are far to much! Do you really believe that much iron is in your other solutions? This would mean about 0,7 grams of iron nitrate hydrate!

You can test for iron with potassium ferrocyanide (for Fe3+) or potassium ferricyanide (for Fe2+). In the presence of iron you will get a blue solution or precipitate ("prussian blue").

Both tests (cyanide-complex and thiocyanate) are very sensitive. Your thulium metal is not 99.999 % pure, so there will be iron in it! This also isn't a usefull method to decide wether you have thulium or something else. There is no reason to believe that it is something else but thulium. You have to find a real test for thulium (in the way it is done for other lanthanides like here).

[Edited on 9-7-2014 by Pok]
View user's profile Visit user's homepage View All Posts By User
blogfast25
Thought-provoking Teacher
*****




Posts: 10340
Registered: 3-2-2008
Location: Old Blighty
Member Is Offline

Mood: No Mood

[*] posted on 9-7-2014 at 08:57


Quote: Originally posted by Pok  
This also isn't a usefull method to decide wether you have thulium or something else. There is no reason to believe that it is something else but thulium.


Wow. Calm down already (what's with the barrage of exclamation marks?)

As far as I can see it's been established it is Thulium. But there are appears to be a small contamination of iron. That appears to be quite common with some Ln elements.

Nothing wrong with investigating the possible source of that contamination. My bet is on the cutting tool.




View user's profile Visit user's homepage View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 9-7-2014 at 09:07


As you can see from some of my mistakes, I am still very much learning. I am an electrical engineer, professionally, and I tinker in lots of stuff and have broad general science knowledge but I have a lot to learn. I wanted to test for iron in order to learn how its done.

I do agree that it is most likely Thulium. There was some doubt for a while because the Thulium sulfate crystals I got do not appear light greenish (at least, I do not perceive it) but then I made the nitrate and chloride salt solutions and they DID have a noticeable green tint so I am satisfied that it is Tm. In any event, this is all about learning and fun.

As for the 100mg iron - yes, I do understand that is a huge amount for this test. If you read my posts again, you'll see that I diluted it 10:1 after reacting it with the nitric acid to make sure all of it was in solution. This is in part because I have a limited ability to measure much less than 100mg accurately. In retrospect, I probably should have diluted it 100:1, but it still served the purpose of showing that the test could detect iron.

I do appreciate your help and the help of everyone here. I am learning a lot.
Quote: Originally posted by Pok  
I don't see a reason for you to test for iron. Thulium is very slightly magnetic as your sample is. This cannot be explained by the very low iron content! Even if it is contaminated with iron, it is very very low as you can see from your test. This low contamination won't lead to such a rather strong attraction to a magnet!

Your 100 mg of iron are far to much! Do you really believe that much iron is in your other solutions? This would mean about 0,7 grams of iron nitrate hydrate!

You can test for iron with potassium ferrocyanide (for Fe3+) or potassium ferricyanide (for Fe2+). In the presence of iron you will get a blue solution or precipitate ("prussian blue").

Both tests (cyanide-complex and thiocyanate) are very sensitive. Your thulium metal is not 99.999 % pure, so there will be iron in it! This also isn't a usefull method to decide wether you have thulium or something else. There is no reason to believe that it is something else but thulium. You have to find a real test for thulium (in the way it is done for other lanthanides like here).

[Edited on 9-7-2014 by Pok]


[Edited on 9-7-2014 by sbreheny]
View user's profile View All Posts By User
kmno4
International Hazard
*****




Posts: 1439
Registered: 1-6-2005
Location: Silly, stupid country
Member Is Offline

Mood: No Mood

[*] posted on 9-7-2014 at 10:03


Mentioned extraction is useful only for comparation of very small amounts of Fe. When concentration is relatively high, no extraction is needed. Very small I mean < 1 &mu;g/dm3 of Fe.
On the picture, solution of SCN complex in water and the same sample + butanol.

Back to topic - without VIS spectrum there is no simple way to check purity of your thulium.
Mentioned paper (DOI: 10.1021/ja02221a007) gives interesting example - even small erbium contamination may give colourless thulium salts solutions (I think it is also valid for Nd contamination).

but.bmp - 502kB




Слава Україні !
Героям слава !
View user's profile View All Posts By User
 Pages:  1    3  

  Go To Top