Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
 Pages:  1  2
Author: Subject: Woo hoo, I built a working ball mill!!!
sdodgen62
Harmless
*




Posts: 12
Registered: 1-1-2012
Member Is Offline

Mood: maniac

[*] posted on 20-5-2012 at 19:58


well you know a joint may have helped but figured the desription would have told what your asking, yes it is flake from scrap yard
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 21-5-2012 at 01:23


You'll need to run your mill for a looong time to get pyro-grade flake from chips ─ the thinnest alufoil when torn to small pieces, can be milled to give fine powder if lead media is used.
And running a mill with the jar open is not a good idea . . .

View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1243
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 27-5-2012 at 16:29


Totally off topic, but what the hell happened to evil_lurker?



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 30-5-2012 at 07:39


Quote: Originally posted by Fleaker  
Totally off topic, but what the hell happened to evil_lurker?


Also, Sauron, not_important, entropy51, Marvin, JohnWW, etc, etc.
They come and they go...some by choice; others are escorted off by the grim reaper.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 30-5-2012 at 13:47


I miss new posts by all of them Magpie, and especially those by entropy51 and Sauron.
Their intelligence, pragatism and wit was/is life-affirming!

View user's profile View All Posts By User
Funkerman23
National Hazard
****




Posts: 411
Registered: 4-1-2012
Location: Dixie
Member Is Offline

Mood: No Mood

[*] posted on 30-5-2012 at 13:59


Quote: Originally posted by hissingnoise  
You'll need to run your mill for a looong time to get pyro-grade flake from chips ─ the thinnest alufoil when torn to small pieces, can be milled to give fine powder if lead media is used.
And running a mill with the jar open is not a good idea . . .

perhaps but with United nuclear out of stock for some time and quite a few others now gone finding that lead( and other types of) media maybe difficult..
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1004
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 30-5-2012 at 16:06


Here's my Frankenstein's monster. Note it's only half done.

Ball Mill smrezied.JPG - 156kB
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 31-5-2012 at 01:15


─ Funkerman, I checked the UN site; they have A/H lead media in stock now!
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 31-5-2012 at 01:26


─ Hyfalcon, your mill looks good and the jar looks well-used; you will though, need rubber or tape on the driver to provide a good grip for the jar.
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1004
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 31-5-2012 at 02:12


The black you see on the jar is rubber based paint.
View user's profile View All Posts By User
 Pages:  1  2