Make pressure tolerant containers! For liquid gases storage, diamond production and other.
What is the best, but more common material for that? On what does it's strength depend? Is it density, mass, melting point, allotrope...? I know that
Anvil cell is one very strong. But, why? What else can I use? Is strength increased by mass and thickness? What people have to know when they wanna
build those containers and reactors?
|
|
|
phlogiston
International Hazard
   
Posts: 1355
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Having trouble with your fusion reactor?
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
|
Bert
Super Administrator
       
Posts: 2751
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Personally, I ALLWAYS use Krell metal for these applications. Some have used transparent Aluminum, but that's a marginal improvised materials choice.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
|
AsocialSurvival
Harmless
Posts: 43
Registered: 8-10-2014
Member Is Offline
Mood: No Mood
|
|
|
|
|
IrC
International Hazard
   
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Quote: Originally posted by Bert  | | Personally, I ALLWAYS use Krell metal for these applications. Some have used transparent Aluminum, but that's a marginal improvised materials choice.
|
If the Krell had used 26 inches of Aluminum Oxynitride instead of their metal Altair IV would still exist and Robbie would still have a job.
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
|
Etaoin Shrdlu
International Hazard
   
Posts: 724
Registered: 25-12-2013
Location: Wisconsin
Member Is Offline
Mood: Insufferable
|
|
Okay, but first I want my infinite nitric acid reactor.
|
|
|
elementcollector1
International Hazard
   
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Actually, I'd like to know just what the standard practice is for high-pressure containers. From what I've discussed with a few professors, welded
steel and sintering aren't going to work very well - so what does that leave?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
|
Brain&Force
Hazard to Lanthanides
   
Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline
Mood: Incommensurately modulated
|
|
This is actually a valid question, unusually enough, if you scale down the requirements from interstellar to temps around 2000 C and a few atmospheres
of pressure.
Diamond anvil cells can produce 300 gigapascals of pressure, but they're not feasible for the amateur. Those are, however, interesting for studying
the different types of ice.
At the end of the day, simulating atoms doesn't beat working with the real things...
|
|
|
HgDinis25
National Hazard
  
Posts: 439
Registered: 14-3-2014
Location: Portugal
Member Is Offline
Mood: Who drank my mercury?
|
|
Quote: Originally posted by Bert  | | Personally, I ALLWAYS use Krell metal for these applications. Some have used transparent Aluminum, but that's a marginal improvised materials choice.
|
I had to google Krell... Damn now I feel bad about my ignorance 
Ontopic, it kind of depends on the pressure you're going to put on it. Diamond isn't produced inside pressurized containres, AFAIK.
Pressurized CO2 extinctors are a fairly good example of relatively high pressure gas containers.
|
|
|
Metacelsus
International Hazard
   
Posts: 2506
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Fire extinguishers are nowhere close to what's considered "high pressure" in research.
https://en.wikipedia.org/wiki/Piston-cylinder_apparatus
https://en.wikipedia.org/wiki/Anvil_press (both for larger samples, a diamond anvil cell is usually used for smaller samples)
[Edited on 10-11-2014 by Cheddite Cheese]
As below, so above.
|
|
|
Imperial
Harmless
Posts: 1
Registered: 17-11-2014
Member Is Offline
Mood: No Mood
|
|
Many lab created gemstones these days are not made in high pressure vessels but rather through other means. For instance, Laser-heated pedestal growth
is able to create extremely pure gem stones of almost any composition several hundred grams+ in just a few hours. Many industrial processes that
produce huge 1-tonne blocks of stones (like huge blocks of sapphire/ruby) do so with basic chemical crystalization techniques over many months in big
chambers. These stones are often far from pure, but pure segments are easily isolated.
There's a reason why diamond necklaces with synthetic diamonds only cost a couple hundred bucks, with it's "natural" counter part costing millions.
The chemical composition is the same, although the synthetic is more chemically pure and therefor more brilliant. These days when people spend tons of
money on jewelry they're doing it more for the rarity/historical factor, knowing their gems were naturally made in the earth.
Believe it or not it can be extremely difficult to produce synthetic gems in the laboratory that mimic their natural earthen counter parts.
We regularly produce synthetic gemstones in our lab for scientific applications. You would be surprised how incredibly hard it is to sell synthetic
but chemically sound gem stones. Because of their synthetic ease they are worth next to nothing outside of the industries that use them for their
chemical properties (optics, glass, touchscreens, those sorts of things).
|
|
|