Molybdenum - how to etch/roughen?
I need to figure out a way to take molybdenum sheet with a smooth surface finish and roughen it. Abrasive blasting hasn't worked all that well. A belt
sander does work OK, but I want to find another solution; a chemical one. There's always the worry of contamination of the metal surface with the
abrasive media in the above two methods.
So what would be a good acid / other chemical to use for etching?
|
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
If you want it hell ass rough I don't think chemical means will be very useful, aside from nasty pitting if you can make it. Getting such a deep
corrosion is going to use a lot of metal, too.
Tim
|
|
|
lordmagnus
Hazard to Self

Posts: 92
Registered: 10-1-2006
Location: Webster, TX
Member Is Offline
Mood: No longer annoyed ( I found a new girlfriend)
|
|
Good luck,
Maybe hydroflouric acid at various dilutions. The old Steel divers airtanks were coated with a few layers of molybdenum t resist corrosion, I don't
think I've ever seen one actually rust
I\'ll kill a man in a fair fight, or if I think he is gonna start a fair fight, or if he\'s bothrn me allot, or if I am getin payed good, or probably
over a good woman.
-Jayne Cobb (Serenity)
|
|
|
chromium
Hazard to Others
 
Posts: 284
Registered: 27-6-2005
Member Is Offline
Mood: reactive
|
|
If you have time to experiment, you may try to use your molybdenum as anode in electrolytic cell with different electrolytes. Some of electrolytes may
appear quite destructive to surface but then again they may just passivate or oxidise surface. Some amount of HF (or maybe just NaF) is probably
needed to get etching to work.
|
|
|