fuckin plastic piece of shit hoses
i almost lost my life right now. was working with a reactor with a heating jacket 210C, heated by mineral oil from the termostat, pumped by 0.5 -1m/s.
and the little fuckin retarded techincian idiot supplied me with a hose that can stand up to 75C.
i dont need to explain what happened next, the hose melted, the oil started bursting all over the lab, i got burns over my chest, the reactor cracked,
the mixture caught fire, my lab coat started to burn, my gloves melted....FUUUUUCK.
im standing in the middle of some 5 m2 of oil around me..
luckily i was fast enough to put out the fire and strip. i hope the burns are not too dangerous, there are only a few blisters, and some part of the
melted glove in my fuckin hand. and not to mention the embarresment when the firemen ran in and found me in my boxershorts and undershirt trying to
put out the fire...
goddamnit, I HATE FUCKIN TECHINICIANS.
sorry for the bitching but i had to let off some steam, since officaly im responcible for this shit....im off to the doc
peace, oil, sand and soap.
[Edited on 13-6-2006 by daeron]
Humans with their brains are like a caveman with a supercomputer. Yes there is a chance that the caveman will use it to calculate the trajectories and
the momentums of the celestial bodies, but the chances are that he will just crack open a coconut with it.
|
|
|
Saerynide
International Hazard
   
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Wow. That sucks. Glad you're ok.
Btw, fire the bastard.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
chochu3
Hazard to Others
 
Posts: 185
Registered: 21-10-2003
Location: South Side Tejas [Cloverland]
Member Is Offline
Mood: Inside looking out
|
|
That's why an authority always over checks the work of a techinician.
\"Abiding in the midst of ignorance, thinking themselves wise and learned, fools go aimlessly hither and thither, like blind led by the blind.\" -
Katha Upanishad
|
|
|
MadHatter
International Hazard
   
Posts: 1264
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Technician
Agreed. Fire the incompetent fuck. Also, with the next technician you get, carefully
review the setup. Glad your OK.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
unionised
International Hazard
   
Posts: 4949
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Fire the guy who didn't train the tech.
|
|
|
Nerro
International Hazard
   
Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline
Mood: Whatever...
|
|
If you do such work it can't hurt to check the items supplied to you, you may want to do that from now on.
Jope you'll be ok though, burns really suck. I once melted a bit of plastic into the skin of my hand, took ages to come off.
#261501 +(11351)- [X]
the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally
courtesy of bash
|
|
|
unionised
International Hazard
   
Posts: 4949
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.
BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire.
|
|
|
Nerro
International Hazard
   
Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline
Mood: Whatever...
|
|
| Quote: | Originally posted by unionised
I hope you are OK and have calmed down enough to see the funny side of
"I HATE FUCKIN TECHINICIANS"
well fuck someone else then.
BTW, if the oil was at 75C when the hose failed, what cracked the reactor and what started the fire. | LOL!
#261501 +(11351)- [X]
the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally
courtesy of bash
|
|
|
daeron
Hazard to Self

Posts: 74
Registered: 26-3-2005
Member Is Offline
Mood: cancerogenic
|
|
thx to all who replied, the person altho she was HOT was fired, so no fucking of technicians there. got burns over my chest and some plastic in my
right arm but otherwise im okay. this was a good lesson.
Humans with their brains are like a caveman with a supercomputer. Yes there is a chance that the caveman will use it to calculate the trajectories and
the momentums of the celestial bodies, but the chances are that he will just crack open a coconut with it.
|
|
|
MadHatter
International Hazard
   
Posts: 1264
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Technician
Ashame she's real HOT ! I'd say she owes you a fuck for the misery she put you through
as a contrite apology to the agrieved.  
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
DeAdFX
National Hazard
  
Posts: 339
Registered: 1-7-2005
Location: Brothel
Member Is Offline
Mood: @%&$ing hardcore baby
|
|
If your going to fuck people at your work place at least make sure that they can give you a promotion otherwise its not worth the time to take out the
knee pads...
[Edited on 22-6-2006 by DeAdFX]
|
|
|
andersderis
Harmless
Posts: 4
Registered: 24-6-2006
Member Is Offline
Mood: No Mood
|
|
fire tha bitch!!!
|
|
|
Adar
Harmless
Posts: 7
Registered: 8-7-2006
Location: Sweden
Member Is Offline
Mood: Having fun with vaseline
|
|
Could you show a picture of the cracked reactor and point out the hose? It could be useful to avoid future mishaps for other people (and be quite
intresting).
|
|
|