Author: Subject: Best Acid that will get rid of rust quickest without harming iron?
gatosgr
Hazard to Others
***




Posts: 237
Registered: 7-4-2015
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2015 at 10:36


I mean that some polymers get corroded from salts(from sea spray). Also the polymer adsorbs? the salts and it turns whitish I don't know how to describe it better.

I'm talking about polyurethane polymers I guess there are many unreacted OH groups left that the salt can attack.


[Edited on 14-6-2015 by gatosgr]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2015 at 11:15


Maybe. Not sure what the SRP of Na<sup>+</sup> has to do with anything though...



View user's profile View All Posts By User
gatosgr
Hazard to Others
***




Posts: 237
Registered: 7-4-2015
Member Is Offline

Mood: No Mood

[*] posted on 14-6-2015 at 13:12


It has something to do with how do you remove the salt that gets into the polyurethane due to open pores from salt corrosion? I'm going slight oftopic but what the heck.

[Edited on 14-6-2015 by gatosgr]
View user's profile View All Posts By User