How to separate silver sulfide nano particle from silver-silver sulfide mixtures...???
View user's profile View All Posts By User
bolbol
Hazard to Others
***




Posts: 162
Registered: 3-1-2015
Member Is Offline

Mood: No Mood

[*] posted on 7-3-2015 at 02:38


According to wikipedia silver sulfide isnt soluble in "acids". So if you have nitric acid then try a small amount and after the reaction of silver is done check out to see if there is anything left. That would be your silver sulfide.
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1403
Registered: 2-9-2012
Location: Back yard staring at stars
Member Is Offline

Mood: Good

[*] posted on 7-3-2015 at 03:30


sulfide - http://en.wikipedia.org/wiki/Sulfide
"Upon treatment with a standard acid, sulfide converts to hydrogen sulfide and a metal salt"

silver sulfide - http://en.wikipedia.org/wiki/Silver_sulfide
"Silver sulfide is insoluble in all solvents, but is degraded by strong acids"

bolbol- Wiki did *not* say it(Ag2S) wasn't soluble in acids, they( acids) degrade the sulfide. it also stated Ag2S *isn't* soluble in solvents. adding acid, that would wreck the nano-particle's that may have been the target compound.. and let off a nice healthy *(cough, wheeze die ) cloud of hydrogen sulfide gas... not a good idea. more or less dangerous depending on actual amounts used, but just take it as dangerous if your not sure.

vibhudharshan - which brings me to another point, a little bit more info from OP would be nice. I understand this is in fundamentals, but that doesn't mean you couldn't tell us a little bit about the way it was made and how much of it you need to clean up.

personally I don't know off the top of my head, what you should do. but I can say, don't add a lot of sulfide salt to a bunch of acid ok! could you make the limiting reagent work in your favor? guess it really depends on how you did it. silver nitrate + sodium sulfide? or more complicated.
View user's profile View All Posts By User
vibhudharshan
Harmless
*




Posts: 4
Registered: 23-2-2015
Member Is Offline

Mood: No Mood

[*] posted on 13-3-2015 at 00:10


sir,
Thank you for your replay .Actually,i supposed to make silver sulfide nanowires based upon a simple chemical synthesis.in this procedure i poured 12.5 ml of thiourea into 2 ml of 0.7% of ammonia solution ,25 ml of silver nitrate solution added into that stirring solution. Eventually i got Ag2S powder with little amount of native silver. i tried to remove silver from that mixture but i couldn't .
Can you please suggest a good procedure to synthesis Ag2S wires using same reagents?
View user's profile View All Posts By User
vibhudharshan
Harmless
*




Posts: 4
Registered: 23-2-2015
Member Is Offline

Mood: No Mood

[*] posted on 13-3-2015 at 00:13


i downloaded the journal paper from 'sciencedirect"named as "Ag2S morphology controllable via simple template-free solution route"
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3016
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2015 at 18:13


Would simply treating (and storing away from light) the Ag2S/Ag mix with H2S remove your unwanted Ag?

The fact that we have nano size particles is probably a plus here in moving the reaction along.

My inspiration is the evident propensity of Silver to tarnish.
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1403
Registered: 2-9-2012
Location: Back yard staring at stars
Member Is Offline

Mood: Good

[*] posted on 17-3-2015 at 20:26


@vibhudharshan : from the papers I read while trying to help a bit, silver sulfide nano-wires were made from sacrificial silver nano-wire templates. so is there a possibility you could continue to convert the silver? I haven't read the paper you mention, but I did search using the reactants you mentioned. this was probably the best match I saw with out knowing which paper you used.

I don't have access to the paper you mention and the abstract doesn't tell a whole lot. could you give a quick breakdown of the process you used?