Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Metal dendrites
Gleb
Harmless
*




Posts: 8
Registered: 23-4-2015
Location: Russia
Member Is Offline

Mood: No Mood

[*] posted on 29-4-2015 at 06:16
Metal dendrites




z0VCbxaK8Zo.jpg - 36kB 8vPwCj26TKc.jpg - 40kB l0RbtbuNmbk.jpg - 32kB Ew4jI5nPgL0.jpg - 35kB GMIJ8zaObG4.jpg - 46kB g5sLnq9NRF4.jpg - 43kB BoBGx5pTync.jpg - 34kB DwKCu85XG1Q.jpg - 70kB 9x2mLtM33ZE.jpg - 38kB AnRpXGnFuWo.jpg - 62kB
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 29-4-2015 at 06:29


Quote: Originally posted by Gleb  

Metal dendrites


Welcome to Sciencemadness. We have a designated thread for pictures like these, I would post them there next time. Overall, great pictures though!




View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1299
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 29-4-2015 at 14:14


How did you do it?



At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
Marvin
International Hazard
*****




Posts: 994
Registered: 13-10-2002
Member Is Offline

Mood: No Mood

[*] posted on 29-4-2015 at 15:37


Electrolysis, the more dilute the solution the more it favours branching. I did this a long time ago but those are way better than I managed. What range of current and concentration are you using Gleb?
View user's profile View All Posts By User
diddi
International Hazard
*****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 29-4-2015 at 17:07


I am assuming Cu and Ag ?



Beginning construction of periodic table display
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 5833
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Possessor of a tidy and organised lab. Now to mess it up again.

[*] posted on 29-4-2015 at 20:17


That last one or the third to last might be tin.
Take a look at the video posted in Pretty Pictures.
Quote: Originally posted by Sulaiman  
I made a video of tin crystals growing by electrolysis in real time,
I think it's pretty. https://www.youtube.com/watch?v=G1sq4hnrBgM
View user's profile View All Posts By User
diddi
International Hazard
*****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 30-4-2015 at 05:22


hmm possibly Sn
would have been nice to have some labels...




Beginning construction of periodic table display
View user's profile View All Posts By User
Gleb
Harmless
*




Posts: 8
Registered: 23-4-2015
Location: Russia
Member Is Offline

Mood: No Mood

[*] posted on 30-4-2015 at 23:06


4, 5, 6 - Cu, sulfate
7 - Ni, sulfate
8 - Pb, acetate
10 - Zn, acetate
1, 2, 3, 9 - Cu and Bi, nitrate
All are concentrated solutions. And high currents (1-2 A)

[Edited on 1-5-2015 by Gleb]

[Edited on 1-5-2015 by Gleb]
View user's profile View All Posts By User
diddi
International Hazard
*****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 1-5-2015 at 00:22


from nitrates?



Beginning construction of periodic table display
View user's profile View All Posts By User

  Go To Top