Gold at the beach?
Okay so today I tried getting gold out of beach sand, but it just left me confused.
I've always noticed this gold flake looking stuff at a certain part of the beach, a sheltered 30m or so. It is only in that area on the beach, which
is several kilometers long. The flakes are among the sand, each piece being 0.5 - 2.5 mm long. It gets more abundant in the sand the deeper it is dug.
Hopefully that made sense.
Today I went out in the storm and gathered about 3 pounds of the sand, and tried panning it out. Despite that gold should be about (9?) times heavier
than the sand, it still didn't settle. In fact, the flakes would be washed to the surface by the water and would deposit ON TOP of the sand. Also, I
pulled some pieces out with tweezers, and rubbed them over white paper. They left long, strong coloured gold streaks, and crumbled.
Is this gold, or what? Its a light flaky solid which crumbles easily. I'm thinking it might be pyrite, since I recovered some from rocks only a few
kilometers away.
|
|
|
Texium
Administrator
      
Posts: 3931
Registered: 11-1-2014
Location: Salt Lake City
Member Is Online
Mood: Triturated
|
|
If it is pyrite, it should react with hydrochloric acid to evolve hydrogen sulfide and yield a yellow iron(III) chloride solution. If it doesn't react
immediately, maybe try warming it a bit. If it is actually gold, that shouldn't do anything to it.
|
|
|
Hawkguy
National Hazard
  
Posts: 326
Registered: 10-10-2014
Location: British Columbia (Canada eh!)
Member Is Offline
Mood: Body is Ready
|
|
Thanks Mate, will do. I have uses for pyrite and for gold, so its a win either way.
|
|
|
j_sum1
Administrator
      
Posts: 5830
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Possessor of a tidy and organised lab. Now to mess it up again.
|
|
Mica is another possibility I think.
|
|
|
hyfalcon
International Hazard
   
Posts: 1004
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Without seeing it, my vote is for mica also. The fact that it floats to the top tells you that.
Pyrite would stay in a layer in the bottom. It's heavier than sand, but lighter than gold would be.
[Edited on 1-9-2015 by hyfalcon]
[Edited on 1-9-2015 by hyfalcon]
|
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
It's mica.
Flaky solid that crumbles easy, not very dense, sparkly appearance, often found on beaches and in streambeds. All of that screams mica. Pyrite has a
black streak, so it's not that either (you might as well test it if you have some acid handy just to be 100% sure).
If it was gold just sitting out in the open, someone would have mined it already!
|
|
|
UC235
International Hazard
   
Posts: 551
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
Sounds like mica or possibly powdered shells from members of the family Anomiidae (Jingle Shells). Pyrite is extremely unlikely since it rapidly
weathers to hydrous iron oxides (it is also quite dense which this is not).
[Edited on 1-9-2015 by UC235]
|
|
|
Morgan
International Hazard
   
Posts: 1574
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Here's an account of mica on the beach.
"The glitter swooshed around in the water like a snow globe, and the metallic flecks, which were softer and flatter than regular sand, stuck to my
skin when I stepped out of the waves. Instead of enjoying some beachside R&R, I found myself panicking."
A Beach So Beautiful, I Thought It Was Polluted
https://figureoneblog.wordpress.com/2013/09/06/a-beach-so-be...
|
|
|
NedsHead
National Hazard
  
Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline
Mood: No Mood
|
|
sounds like pyrite, they don't call it fool's gold for nothing
[Edited on 2-9-2015 by NedsHead]
|
|
|
elementcollector1
International Hazard
   
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Yep, it's mica. I've run into this stuff on Oregon beaches enough to know what it is...
Elements Collected:52/87
Latest Acquired: Cl