Author: Subject: mineral oil
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 11-10-2015 at 16:05
mineral oil


Needing some mineral oil with a boiling point of 400±20°C I assumed that I could obtain this by fractional distillation. My first attempt was to use some old (>20 yrs) Albertson's USP that I had on hand. Using a 200mm Vigreux column I did manage to distill off some of the light ends until the distillate temperature reached about 310°C. I didn't want to go any higher fearing I might damage my mantle. Also the pot liquid and the condensate had taken on a translucent yellow color.

My next attempt was to obtain some fresh mineral USP oil from Target where their website said it was "extra heavy." Here I used vacuum fractionation to keep the temperature down. My pressure was 0-0.5 mmHg and the distillate bp was 160°C. But the Claisen adapter and the lower 3rd of the column were flooded so this data may not be of any value.

The mineral oil seems "heavy," ie, viscous, so I think I'll just use it "as is." It is dirt cheap at $2/pint.

You can see my distillation set-up below. The Claisen allowed use of an ebulliator, necessary because of severe bumping. Under the Al foil are fiberglass blankets.





mineral oil fractionation - insulated.jpg - 84kB mineral oil fractionation - undressed.jpg - 81kB




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 508
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 12-10-2015 at 06:33


Mineral oil turns yellow after heating to 200 degrees Celsius for me too. This is not some dirt cheap mineral oil, this is analytical reagent grade lab stuff. No idea why though.
View user's profile View All Posts By User
m1tanker78
National Hazard
****




Posts: 685
Registered: 5-1-2011
Member Is Offline

Mood: No Mood

[*] posted on 12-10-2015 at 07:35


Same here, I can always count on mineral oil turning yellow, orange-brown or even black depending on how much heat I apply and for how long. If you leave the 'burnt' oil in a sep funnel or any other container for a few days, undistrurbed, the colored matter will settle at the bottom and yield crystal clear oil above it. Most of the gunk can be flushed from the sep funnel or carefully removed from a beaker by decanting or syphoning.

Magpie, why did you run a distillation if you only wanted the higher boiling fraction? I routinely prepare batches of mineral oil for storing sodium. Part of that entails removing traces of water and other low-boiling stuff that may be in there. I heat the snot out of the batch (well beyond the smoke point) and then do the procedure I outlined in the above paragraph.

Were you wanting to collect the lower boiling fractions for analysis?




Chemical CURIOSITY KILLED THE CATalyst.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 12-10-2015 at 08:12


Quote: Originally posted by Magpie  

The mineral oil seems "heavy," ie, viscous, so I think I'll just use it "as is."



Upon reflection I'm going to have to do better at isolating a fraction boiling at 400±20°C. I need this fraction as a diluent for making 2-octanol. During the synthesis the octanol is distilled off. I don't want any light minera oil ends contaminating it.

Thanks to both of you for the input on yellowing. And thank you tank for your method on obtaining a heavy fraction. On my initial attempt with the Albertson's oil I definitely accomplished some separation as it was evident from the difference in viscosity of the two fractions.

mineral oils.jpg - 90kB




The single most important condition for a successful synthesis is good mixing - Nicodem