Author: Subject: Making bismuth crystals, but they won't oxidize.
esgeroth
Harmless
*




Posts: 4
Registered: 1-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 24-2-2016 at 15:17
Making bismuth crystals, but they won't oxidize.


Anyone here do anything with bismuth? I don't know if this is the best place to get help with this but I sure don't know of any forums dedicated to bismuth so here it goes.

My son and I have been having lots of fun making crystals from different metal salts and other things. So we wanted to try making some crystals from bismuth due to its very colorful oxidation layer. I bought a small amount on ebay and we made a couple of small crystals that looked great. I wanted to make something a little bigger so then I bought 5 pounds of bismuth that was advertised as 99.99% pure.

I melted it down, let it cool for a few minutes, and poured it out. It left some crystals in the container but did not oxidize so it does not have any color to it at all. Just silver. Also some of the crystals are a bit different looking as well. Some are forming triangles instead of squares and there aren't as many of the larger cube shapes. I've tried melting it several times with the same results.

From any of the videos I have watched it seems that this is pretty easy to do. Is it likely that my bismuth is contaminated with something else? I got it from a reputable dealer that specializes in bismuth alloys. But the bismuth I bought should be 99.99% pure. I don't think it would have been contaminated when I melted it since it went straight from the bag it came in into a ceramic baking dish I had been using to melt it.

So does anyone have any tips on working with this stuff or should it be easier than this?





P_20160128_214827.jpg - 2MBP_20160223_184306.jpg - 1.5MB
View user's profile View All Posts By User
crystal grower
National Hazard
****




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 25-2-2016 at 01:00


I'm not sure if it's this case but I was making bismuth crystals and results were really nice.But after I accidently contamined my bismuth with very little amount of tin, every attempt ended similarly to yours.
Now I will probably buy new bismuth and try it again.
This is one of my best bismuth crystals (the "price 20€" doesn't belong to crystal it's just coincidence if it interests anyone:D).

P2222505.JPG - 1.7MB



[Edited on 25-2-2016 by crystal grower]




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
esgeroth
Harmless
*




Posts: 4
Registered: 1-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 26-2-2016 at 14:19


How did you contaminate your bismuth? Was it just from the container it was in? Did you see the small triangular crystals as well? It sure seems like that's what has happened to mine but it went straight from the bag it came in into the ceramic dish I used to melt it.

Anyway, here's some of what I was able to get before I bought this 5 pound block. I just wish I could replicate it now.

P_20160224_210447.jpg - 1.1MBP_20160224_210528.jpg - 897kB
View user's profile View All Posts By User
crystal grower
National Hazard
****




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 27-2-2016 at 01:49


No, when I bought bismuth it was very pure.
It´s long story how i have contamined them so nevermind :D.
at least it was only 250g bismuth that is contamined.
In the first image you can see nice crystals of pure Bi.
the second one is contamined bismuth (and yes, there are triangles as u said).

P2222535.JPG - 2MBBi+Snup.JPG - 576kB




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 29-2-2016 at 07:20


hkparker (another SM member) and I talked about this a while back - he had the same problems you are having. He sent his Bi to someone to get it assayed and it did indeed come back as contaminated with a significant amount of tin. I believe he did some experiments and the amount of tin necessary to inhibit oxide formation was very low. So your bismuth may be lower purity than advertised! Purity has a huge impact on oxide colors and crystal formation. My 99.99% Bi forms lovely blues and greens, but my 6N (99.9999%) gets into reds and yellows. Really beautiful, but too precious to experiment with!
View user's profile Visit user's homepage View All Posts By User
esgeroth
Harmless
*




Posts: 4
Registered: 1-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 29-2-2016 at 08:57


Yeah, that's the same type of crystals as I have been getting from this stuff. It definitely seems like it must be contaminated. I don't see where I could have introduced anything into it since I melted it in a ceramic container. Plus its probably a lot harder to contaminate 5 pounds of the stuff rather than 250g. I asked the seller about it and he even sent me the analysis from their distributor certifying it as 99.99% pure.
Is it expensive to get something like this assayed? Where can this be done?
View user's profile View All Posts By User