Hello!
I've been trying to develop some type of super capacitor, most likely using graphene or a graphene alloy of some sort within it. I came across a
youtube video .. here's link:
https://www.youtube.com/watch?v=7l3CAKJemb4
suggesting a capacitor with an ionic liquid electrolyte called BMPDCA (1-butyl-1-methylpyrrolidinium dicyanamide. Claims of voltage between 4-10v
which is outstanding.
From what I can read as the journal for this capacitor is briefly flipped over infront of the camera, the carbon based electrodes are passivated in
the ionic liquid, which causes a dielectric layer of DCA polymer to form on the electrode surface.
My question is this... Can the full paper be found anywhere, because I don't wanna pay 50$ for it or whatever it costs, and 2: does anyone know a
method or source for the ionic liquid? (home chemist with a fair bit of glass)
again, the ionic liquid is bmp (1-butyl-1-methylpyrrolidinium) with a dca (dicyanamide) anion.
Hope someone has a clue!
|
|
|
PHILOU Zrealone
International Hazard
   
Posts: 2880
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
For your document request, maybe ask in the "Reference" section of the forum...
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
|
Nicodem
|
Thread Moved 29-2-2016 at 09:41 |
Nicodem
Super Moderator
     
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
1-Butyl-1-methylpyrrolidinium dicyanamide is available commercially.
Please limit article requests only in the Reference section.
…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being
unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their
scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)
Read the The ScienceMadness Guidelines!
|
|
|
localbroadcast
Harmless
Posts: 19
Registered: 11-5-2013
Member Is Offline
Mood: No Mood
|
|
sorry its been a long time since posting in this forum at all. my appologies. When you say it is commercially available.. Do you mean that it is
available through chemical suppliers, or do you mean it is available in some type of over the counter solution, like a dish washing detergent or hair
gel. I ask because the price difference is astonishing between the two sources for certain reagents.
That is why I am asking of a known otc friendly synth method.. Of course I could buy the stuff if I wanted to, but that's no fun for anybody! If I
have to pay retail for everything, im never gonna reach the 20000 jigawatt barrier.
|
|
|
IrC
International Hazard
   
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
http://www.emdmillipore.com/US/en/product/1-Butyl-1-methylpy...
$147 for 25 gm.
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
|