Extracting Butyl Rubber
I mixed Butyl Rubber Sealant with naphtha and stirred this heterogeneous mixture to form a more or less homogeneous mixture so that
the butyl rubber content of the sealant may be dissolved by the maphtha solvent. I then allowed the other contents of the sealant to settle to the
bottom of the container and then repeated the mixing process several times to make certain all of the butyl rubber content would dissolve into the
solvent. This was done over a 2 day period. I then decanted the liquid portion of the mixture into another container, this liquid is not clear like
naphtha by itself but somewhat opaque, presumably due to the dissolved butyl rubber that is suspended in the solvent. Now the problem is that the
naphtha solvent is refusing to evaporate. How can I cause the solvent to evaporate so that I can recover the pure butyl rubber? Any suggestions?
|
|
|
nitro-genes
International Hazard
   
Posts: 1029
Registered: 5-4-2005
Member Is Offline
|
|
Fastest is precipitation by the addition of 50% acetone....
|
|
|
Frontier9
Harmless
Posts: 16
Registered: 3-7-2006
Member Is Offline
Mood: No Mood
|
|
Thanks for the info nitro-genes; I'm assuming by "addition of 50%", I need to add a volume of acetone that is equal to 50% of the volume of the
solution that is already in the container. Am I correct in this assumption? Furthermore, I am surprised that acetone which itself is a
solvent would cause the polyisobutylene to precipitate out of the solution. What's up with that? Lastly, what
about increasing the temperature of the solution by the addition of heat, would this cause the naphtha solvent to evaporate?
|
|
|
stricnine
Harmless
Posts: 21
Registered: 21-12-2005
Location: Down South
Member Is Offline
Mood: Hard on... working!
|
|
Try applying vacuum. I have a simple water aspirator that reduces the pressure down to the vapour pressure of water. It will take a lot of water
running for a couple of hours (or days!), but it surely will work.
Enjoy!