PVC ducting


Hello, I have been constructing a fume hood so that I can do more inside my lab/shed. The housing is wood, with Plexiglas for the front. The air is being pulled by 2 explosion proof bilge fans outside through some PVC ducting. Does this sound alright for general chemistry? specifically will the presence of nitric or sulfuric acid vapors cause damage to the ducting? I want to do some nitrating of cotton and such in there.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2505
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 7-11-2016 at 06:36


It should be OK; just make sure to periodically inspect it.



As below, so above.
View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 7-11-2016 at 07:39


PVC is rated for use with sulfuric acid of any concentration less than "fuming" at room temperature, and is considered moderately resistant to nitric acid up to 70%. Further, the actual exposure of PVC from fumes is slight (quite different from using it as a storage container).

See:
http://www.calpaclab.com/pvc-polyvinyl-chloride-chemical-com...

What PVC is most vulnerable too is some powerful solvents, principally acetone, halogenated hydrocarbons, and aromatic hydrocarbons.

I would expect though that any solvent vapor would simply render the PVC surface temporarily soft and sticky, from which it would recover after the solvent evaporates off (this what happens when you smear it with purpose-made PVC solvent). PVC of every schedule has thick walls, so any chemical attack from vapor would be hard pressed to undermine its integrity.




About that which we cannot speak, we must remain silent.
-Wittgenstein

Some things can never be spoken
Some things cannot be pronounced
That word does not exist in any language
It will never be uttered by a human mouth
- The Talking Heads
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 7-11-2016 at 08:09


Sounds great !

My 'hood ducting is PVC and works fine.




View user's profile View All Posts By User