symboom
International Hazard
   
Posts: 1133
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline
Mood: Doing science while it is still legal since 2010
|
|
Vandium pentoxide substitute
Vandium pentoxide
Used in oxidizing sulfur dioxide to sulfur trioxide
Oxidizing sugar to oxalic acid
Very useful catalysis with out using preciius nitric acid as one to see but could chromium oxide be substituted in some of reactions as these or
possibly manganese dioxide or cerium oxide
|
|
|
Texium
|
Thread Moved 29-11-2016 at 06:23 |
Meltonium
Hazard to Self

Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline
Mood: Fluorinated
|
|
No; if those could be used as a substitute catalyst, they would probably be used in industry more often. I'm just postulating, though, I don't know
for certain.
|
|
|
learningChem
Hazard to Others
 
Posts: 182
Registered: 21-7-2011
Member Is Offline
Mood: No Mood
|
|
>could chromium oxide be substituted
Maybe. See patent US1787416
[Edited on 30-5-2018 by learningChem]
|
|
|
DavidJR
International Hazard
   
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Cerium is even harder to get...
|
|
|
XeonTheMGPony
International Hazard
   
Posts: 1601
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
just dissolve a few old sockets as they are usually drop forged vanadium.
|
|
|
Corrosive Joeseph
International Hazard
   
Posts: 914
Registered: 17-5-2015
Location: The Other Place
Member Is Offline
Mood: Cyclic
|
|
Pottery suppliers.........
https://www.axner.com/vanadium-pentoxide.aspx
https://www.bathpotters.co.uk/vanadium-pentoxide/p1786
/CJ
Being well adjusted to a sick society is no measure of one's mental health
|
|
|
NEMO-Chemistry
International Hazard
   
Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline
Mood: No Mood
|
|
I cant understand the difference in price between there and here. It isnt a small amount we are talking many many times the price.
I tried to get hold of sum at christmas from pottery places, all had sold out of small amounts, but even then 200g was well over £80.
I thought i had got some cheap but i get two chemicals always mixed up name wise, no idea why but hey ho, i ended up with 500g of the wrong one .
I need to go check now incase i have mixed them up again!!
Looking at the prices on the pottery site there, its way cheaper than we get.
The other bad one at the moment is chlorinated solvents, i found chloroform for sale at a good price (for uk), but the rub was the postage was an
extra £45.
There seems to be a big push towards 'green' solvents, even the universities are switching over.
Sorry i am waffling again
|
|
|
walruslover69
Hazard to Others
 
Posts: 207
Registered: 21-12-2017
Member Is Offline
Mood: No Mood
|
|
Catalysts are really finicky things and the reasons why some compounds act as catalysts and other closely related compound don't or have very big
differences in efficiency usually lies in some part of the mechanism. Its usually pretty hard to reliably choose a substitute catalyst without diving
into the weeds or relying on literature sources for experimental or computation data.
|
|
|
weilawei
Hazard to Others
 
Posts: 130
Registered: 3-12-2017
Member Is Offline
Mood: No Mood
|
|
My understanding is that vanadium pentoxide is often plated on a support from a solution of ammonium metavanadate. The price is essentially the same.
$41 for 100g, $160 for 500g from HiMedia.
|
|
|
woelen
Super Administrator
       
Posts: 7774
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
The element vanadium is quite rare and it is not easily purified. The metal also is quite expensive and this of course also makes compounds of the
metal quite expensive. I myself have V2O5 and also some VOSO4. Both are quite expensive, I paid appr. EUR 25 for 100 grams of V2O5, but that is quite
a few years ago and I paid more than EUR 40 for 100 grams of VOSO4.xH2O.
|
|
|
Hasz
Harmless
Posts: 1
Registered: 31-5-2018
Member Is Offline
|
|
I purchased ~200g for about $20 from a pottery company near me. eBay has a decent selection, at least in the US.
The dust is also surprisingly toxic -- much more than just eating the stuff.
|
|
|
wg48
International Hazard
   
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Apparently there are vanadium pentoxide lithium batteries. https://www.rapidonline.com/Panasonic-VL2330-1HFE-50mAh-Rech...
I cannot find any construction info on them. Perhaps a source vanadium if there are more than button cells in circulation.
Anyone got any info on them or links?
|
|
|
battoussai114
Hazard to Others
 
Posts: 235
Registered: 18-2-2015
Member Is Offline
Mood: Not bad.... Not bad.
|
|
Maybe, but certainly at the expense of selectivity and conversion.
For instance I spent some time looking into V2O5 alternatives when I was looking into ways of converting naphthalene into more interesting molecules
and I found that a few different transition metal oxides would work for the oxidation to phtalic anhydride, but all were less effective in almost all
aspects (main runner-up being MoO3 IIRC).
Vanadium as in pure Va or Cr-Va Steel?
[Edited on 1-6-2018 by battoussai114]
Batoussai.
|
|
|
AJKOER
Radically Dubious
   
Posts: 3016
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
A substitute catalyst is NO2, reaction:
NO2 + SO2 = NO + SO3
NO + 1/2 O2 --> NO2
For a net reaction of:
SO2 + 1/2 O2 --NO/NO2--> SO3
See comments and references at http://www.sciencemadness.org/talk/viewthread.php?tid=83459 .
[Edited on 5-6-2018 by AJKOER]
|
|
|
XeonTheMGPony
International Hazard
   
Posts: 1601
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by battoussai114  | Maybe, but certainly at the expense of selectivity and conversion.
For instance I spent some time looking into V2O5 alternatives when I was looking into ways of converting naphthalene into more interesting molecules
and I found that a few different transition metal oxides would work for the oxidation to phtalic anhydride, but all were less effective in almost all
aspects (main runner-up being MoO3 IIRC).
Vanadium as in pure Va or Cr-Va Steel?
[Edited on 1-6-2018 by battoussai114] |
I am not so sure now, based off the wording you'd think chrome plated vanadium, Guess I'll find out when I get around to dissolving them. they simply
say "Drop forged Vanadium"
|
|
|