Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 1-3-2017 at 03:38
Unusual mystery item


This thing here is the dandest thing. It is finely cut black stone, very heavy and has two electrical fittings to it where it would appear something sits. Never seen a bit of kit made from stone and the two electrical contacts go to those banana type connectiobs.

IMG_1459.JPG - 1008kBIMG_1460.JPG - 896kB




View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2017 at 03:43


anti-vibration base for a speaker? Would keep the bass from rattling.
View user's profile View All Posts By User
Texium
Administrator
Thread Moved
1-3-2017 at 08:45
Lambda-Eyde
National Hazard
****




Posts: 860
Registered: 20-11-2008
Location: Norway
Member Is Offline

Mood: Cleaved

[*] posted on 1-3-2017 at 11:35


This reminds me of those granite blocks used in machine shops as a plane reference, they're called surface plates (though this one is quite thick, hardly a 'plate'). Useful for doing precise measurements and checking squareness.



This just in: 95,5 % of the world population lives outside the USA
Please drop by our IRC channel: #sciencemadness @ irc.efnet.org
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1787
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 1-3-2017 at 12:54


Can the metal lid be removed?
Can you measure any resistance between the wires? Could be a heating block for some apparatus.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2198
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 1-3-2017 at 14:00


Looks like part of a high voltage spark gap, but the
parts that attach to make the gap are missing.

It could also have been a test sample of some kind
but the positioning is wrong for the electrodes.
View user's profile View All Posts By User