Sulaiman
International Hazard
*****




Posts: 3110
Registered: 8-2-2015
Location: UK ... on extended Holiday in Malaysia
Member Is Offline


[*] posted on 21-5-2017 at 04:32
Celite filter aid = diatomaceous earth (DE)


I have just been looking at DE on eBay,

Apparently the darker marine DE has heavy metal content,
so I was looking at the 'purer' fresh water white DE;
http://www.ebay.co.uk/itm/1Kg-Diatomaceous-Earth-DE-Pure-Whi...

Typical Chemical and Physical Analysis:
SiO2 94.2%,
Al2O3 2.5%,
Fe2O3 0.9%,
CaO 0.5%,
K2O 0.4%,
SO3 0.4%,
MgO 0.3%,
P2O5 0.3%,
Na2O 0.2%,
TiO2 0.2%,
Mn2O3 0.1%,
Specific Gravity 1.99,
Apparent Density 2.18,
Moisture 8.3%,
Water Absorption 90.9%,
Loss on Ignition 3.34%,
Porosity 64.5%,
Oil Absorption (30 mins) 58.0%,
Oil Absorption (72 hours) 66.3%,
Particle Size 400 mesh (<37 microns)

I have two questions;

1) does this look suitable ?

2) as it is DE rather than branded Celite, should I process this DE in any way before use ?

It seems odd to filter my reagents through such a chemical mix.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3439
Registered: 15-10-2015
Member Is Offline


[*] posted on 21-5-2017 at 04:49


If you need something analytical grade, it's probably best to just buy some Celite.

That stated, you can improve the quality of that diatomaceous earth with acid washes and drying it at extremely high heat. Actually, I think that's how they make Celite: http://www.sigmaaldrich.com/chemistry/chemical-synthesis/lea...

[Edited on 21-5-2017 by JJay]




View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 4727
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 21-5-2017 at 06:59


One approach is to wash the stuff, just before you use it, with whatever you are filtering.
So, if you are about to filter a solution of something in ethanol, you wash the celite with ethanol before use.
Similarly, you acid wash it before filtering an acid solution.
(I'd not recommend it for strongly alkaline materials)
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 21-5-2017 at 09:06


FYI I bought my Celite at a swimming pool supply store. Only problem is I had to buy a 25 lb bag. It's cheap though.

It's used with swimming pool filters for the same purpose it's used in the lab.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
mr.crow
International Hazard
*****




Posts: 884
Registered: 9-9-2009
Location: Canada
Member Is Offline

Mood: 0xFF

[*] posted on 21-5-2017 at 10:11


The kind you use for killing bugs is NOT suitable for filtering. It turns into goop and the water turns brown.



Double, double toil and trouble; Fire burn, and caldron bubble
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3110
Registered: 8-2-2015
Location: UK ... on extended Holiday in Malaysia
Member Is Offline


[*] posted on 21-5-2017 at 10:17


Thanks for all the guidance,
I'll buy the lot that I pointed to and acid-wash it.
I'm guessing HCl then HNO3




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3439
Registered: 15-10-2015
Member Is Offline


[*] posted on 21-5-2017 at 11:09


I've used the bug killing kind before without incident, but I'm sure it does depend on exactly what kind you get.



View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1350
Registered: 2-9-2012
Location: Back yard staring at stars
Member Is Offline

Mood: Good

[*] posted on 21-5-2017 at 14:31


Wow is spendy 1kg for 6.71£ !! The swimming pool stuff is cheap like magpie says. 19$ for 25# last time around for me. Just got the pool filter all cleaned up and epoxy for some repairs. Spent little under a 100$ on chlorine and acid to boot( 25# trichloro, 2gal muriatic). Nice to have stuff around for experiments, as the beast always needs chlorine and I get to buy in bulk, but honestly I'd say <1% is ever used hobby wise.