Thermolyne 1400


we were donated a thermolyne 1400 furnace, it looks very handy but im curious if anyone happens to know exactly what the heating wire is that it uses...
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1243
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 16-2-2007 at 21:56


What type of furnace is it? If it's a 1400C tube furnace or muffle furnace then it probably uses a high performance nickel chromium element. Most resistance elements are NiCr up until 1400-1500C where molybdenum disilicide, SiC, and graphite are the ones of choice.



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
Chemist514
Hazard to Self
**




Posts: 68
Registered: 12-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-2-2007 at 02:40
Muffle furnace...


Its got a cool door that slides down, suppose to top out at 1200 C, Think i can replace the wire with a dryer heating element? lol, sad but im serious...
The pyrometer works, and the refactory bricks seem intact, just the wire is broke in several places, (I think some freak boiled acid in it.)
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 17-2-2007 at 03:28


Nichrome won't do much more than 1200C. If the length is right, sure.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 17-2-2007 at 05:19


Contact Thermolyne for a relacement heating element.

Anything else and you are asking for trouble.

Give them all the details from the ID plate on the furnace probably at rear. Serial number, model number, volta, amps, watts, everything.

I have withdrawn my earlier remark, as based on your reply I was mistaken..

[Edited on 17-2-2007 by Sauron]
View user's profile View All Posts By User
Chemist514
Hazard to Self
**




Posts: 68
Registered: 12-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-2-2007 at 09:44
ouch.


not quite like that, I had been talking to a machinist about his plans for a burnout oven... I was aware of its condition, saved me from making pretty much the exact same box in the plans.. i was curious though if all items that use heating wire elements used the same thing, in which case i just replace the wire and nothing else. as is, ill go through rebricking 1" with the plans wiring. I just never did anything refractory and wanted to save as much time as possible.

I take out the trash as my job for the labs.. so either way, id have it. heh.

All the best peeps.
View user's profile View All Posts By User
Chemist514
Hazard to Self
**




Posts: 68
Registered: 12-5-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-2-2007 at 09:45


12AX7 : much thanks sir. I use the same gauge wire at same length and its gonna be close, baring anomolies with exact alloy, but one must be realistic. many thanks.

[Edited on 17-2-2007 by Chemist514]