Author: Subject: 1000ml Beakers that i touch explode
Deluxbert
Harmless
*




Posts: 13
Registered: 24-4-2017
Member Is Offline

Mood: Skurr Skurr

mad.gif posted on 27-1-2018 at 17:17
1000ml Beakers that i touch explode


So i seem to be cursed because i have the great luck of constantly breaking 1000ml beakers. Just today I was drying up some iron oxide in a beaker and it just friggin popped. At 150C......
What a joke. How can it be that the vigreux i fixed myself by melting glass shards from bottles (not even boro) into the hole of a shattered finger holds up (done with a shitty torch it even has tons of cracks but no leakage...) but 1000ml beakers just explode in my hands on contact...

First 1L beaker i had exploded in my hands. It wasnt even warm or anything. It was on the hotplate for some time and then i poured off the liquid in it (Water) and let it cool. I had it in my hands (wasnt even noticably warm) and it just cracked when I added some tap water for cleaning.

What am i doing wrong. How can it be that nothing breaks for me no matter how badly i treat them but the 1L just friggin crack to hell. :mad:

Is there something like a prayer or ritual I am missing to keep 1L beakers from exploding.
And no im not using cheap craptastic beakers. First one was a schott, last one was a simax.
But some friggin how chinese crapglass 100-500ml beakers take the same stuff without even taking a scratch.
In my chemist time I only broke one thing that wasnt a 1L beaker :a vigreux (not the one i repaired that one was dead on delivery) But that one broke because a gosh darn metal bar dropped 1m on it.

6 1L beakers and counting.
I think i need to quit buying 1L beakers alltogether and just use flat round bottoms or erlenmeyers....

[Edited on 28-1-2018 by Deluxbert]
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 27-1-2018 at 18:12


Quote: Originally posted by Deluxbert  
So i seem to be cursed because i have the great luck of constantly breaking 1000ml beakers. Just today I was drying up some iron oxide in a beaker and it just friggin popped. At 150C......
What a joke. How can it be that the vigreux i fixed myself by melting glass shards from bottles (not even boro) into the hole of a shattered finger holds up (done with a shitty torch it even has tons of cracks but no leakage...) but 1000ml beakers just explode in my hands on contact...

First 1L beaker i had exploded in my hands. It wasnt even warm or anything. It was on the hotplate for some time and then i poured off the liquid in it (Water) and let it cool. I had it in my hands (wasnt even noticably warm) and it just cracked when I added some tap water for cleaning.

What am i doing wrong. How can it be that nothing breaks for me no matter how badly i treat them but the 1L just friggin crack to hell. :mad:

Is there something like a prayer or ritual I am missing to keep 1L beakers from exploding.
And no im not using cheap craptastic beakers. First one was a schott, last one was a simax.
But some friggin how chinese crapglass 100-500ml beakers take the same stuff without even taking a scratch.
In my chemist time I only broke one thing that wasnt a 1L beaker :a vigreux (not the one i repaired that one was dead on delivery) But that one broke because a gosh darn metal bar dropped 1m on it.

6 1L beakers and counting.
I think i need to quit buying 1L beakers alltogether and just use flat round bottoms or erlenmeyers....

[Edited on 28-1-2018 by Deluxbert]

Buy 900ml ones
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 27-1-2018 at 23:19


I have broken every beaker in my beaker set except for the 50 mL at least once. The 1000 mL spontaneously developed a star crack while sitting on a counter holding some lukewarm solution. But the 100 mL usually breaks within a few weeks every time it is replaced, whether it is dropped, crushed, struck, or exposed to ridiculous temperature extremes.

The 50 mL has never broken, perhaps because I usually use a test tube or a vial instead. The last three pieces of glassware I've broken have all broken while I was cleaning them.




View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6477
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 28-1-2018 at 00:16


My 1000s are my favourite for breaking. Right now I have one sitting in my freezer in pieces. I put it there when I was halfway through some iodine recovery and had to attend to real life. It was still ok the next day when the small amount of water in it had frozen. But it was not ok some time between day 6 and day 7.
Darned annoying really. They cost a few bucks at that size. But then they cost a small fortune to have shipped.




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 28-1-2018 at 00:44


1L is the only size i've never broken, probably because they don't get used much.

Cleaning up is the main cause of glass breakage around here too.




View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 28-1-2018 at 01:04



[/rquote]Buy 900ml ones[/rquote]

Good practical advise LOL
View user's profile View All Posts By User
Deluxbert
Harmless
*




Posts: 13
Registered: 24-4-2017
Member Is Offline

Mood: Skurr Skurr

[*] posted on 28-1-2018 at 04:22


Quote: Originally posted by wg48  

[/rquote]Buy 900ml ones[/rquote]

Good practical advise LOL


Yeah i do think i will only go for 950ml ones because man it sucks having to spend so much on stuff that will prolly break
View user's profile View All Posts By User
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 28-1-2018 at 04:44


It might be an idea to work in smaller batches, I haven’t got any glassware with a capacity exceeding 250mL with the exception of a 500mL Erlenmeyer that I never use. The only ones I’ve broken was when I started out and as a result of too fast heating - in fact I attempted to ‘fire cut’ (burning an ethanol soaked string wrapped around the glass then dumping into water) a broken 50mL separatory funnel and it didn’t even crack when immersed in cold water!



In chemistry, sometimes the solution is the problem.

It’s been a while, but I’m not dead! Updated 7/1/2020. Shout out to Aga, we got along well.
View user's profile View All Posts By User
Texium
Administrator
Thread Moved
28-1-2018 at 07:18
highpower48
Hazard to Self
**




Posts: 96
Registered: 30-10-2014
Member Is Offline

Mood: No Mood

[*] posted on 28-1-2018 at 08:05


Hmmmm, maybe use plasticware. Can't use for heat but lot of uses to have around. Best part you can get a whole selection of plasticware beakers for less than price of one glass 1000ml beaker. Cheap enough that you can call them disposable. ;)
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-1-2018 at 09:26


Quote: Originally posted by highpower48  
Hmmmm, maybe use plasticware. Can't use for heat but lot of uses to have around. Best part you can get a whole selection of plasticware beakers for less than price of one glass 1000ml beaker. Cheap enough that you can call them disposable. ;)


Yes you can, fischer do some. they gave away some freebees with a box of plasters. I forget the name of the plastic but I have a beaker, it takes heat upto 130C i think
Nalgene or something like that its called
View user's profile View All Posts By User
Chemi Pharma
Hazard to Others
***




Posts: 353
Registered: 5-5-2016
Location: Latin America
Member Is Offline

Mood: Quarantined

[*] posted on 28-1-2018 at 09:50


@Deluxbert, try to avoid warm the beckers directly on the top of hotplates surfaces. The glass they were made is too thin, even they're borosilicate made. Any thermal shock can break them easily.

Instead, try to put them inside a metal recipient (aluminum, stainless steel, or everything similar) plenty of water to warm it until 100ºC or motor oil (for baths until 250ºC). The recipient must to be in contact with the hot plate, nor the becker.

When finished and the temperature have gone down, pick up the becker with gloves, not with your bare hands to avoid static eletricity and put it over a non metal surface, or paper towels, never directly over the bench to avoid thermal shock and breakage of the glass.

If you do that and the beckers still breaking down, sorry, but you need to bless yourself in a hurry, cause you're certainly cursed (lol);)
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2324
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 28-1-2018 at 15:00


Which brings us to a topic, I have been wondering about.

Coffee pots. Tough durable. Can take some heat, yet seldom break.

Well, turns out, some common brands.....are borosilicate glass.

https://www.amazon.com/HIC-Pour-Over-Coffee-Borosilicate-Sta...

https://www.amazon.com/Pour-Over-Slow-Coffee-Maker/dp/B0739W...

I'm gonna keep my eyes open at the local garage sales, and thrift stores.

[Edited on 28-1-2018 by zed]
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6477
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 28-1-2018 at 15:23


A proportion of my beakers are repurposed coffee plungers.
No problems thus far.




View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-1-2018 at 15:47


Fischer did a shit job by the look of it. I got three beakers off them. The link to free beakers was posted on the forum!! They sent out the beakers and a set of plasters!!

Some even goto 250c !

https://www.thermofisher.com/uk/en/home/life-science/lab-pla...
View user's profile View All Posts By User
Rhodanide
Hazard to Others
***




Posts: 348
Registered: 23-7-2015
Location: The 80s
Member Is Offline

Mood: That retro aesthetic

[*] posted on 29-1-2018 at 06:17


Beakers are nothing compared to specified glassware. You can buy a set of shiny new beakers for a quick buck, but when we're talking about distillation adapters and such...

I thought I'd be smart and let my adapters sit in cool water overnight after I did my second WFNA run. Seeing as it was winter and it's cold as all shit here in Maine, that was a big mistake. Came back in the morning to find my beautiful, delicate, ever-so-useful-but-not-anymore-because-f*ck-ice, distillation adapters... all caked in solid ice, broken into three pieces each. Needless to say, my reaction was similar to that of Tom Cruise's in "Rain Man". Except, replace the sand with snow.
https://www.youtube.com/watch?v=XRjoCb2a_nk




View user's profile View All Posts By User
Vosoryx
Hazard to Others
***




Posts: 282
Registered: 18-6-2017
Location: British Columbia, Canada
Member Is Offline

Mood: Serial Apple Enjoyer

[*] posted on 29-1-2018 at 10:06


Quote: Originally posted by Tetra  
...
I thought I'd be smart and let my adapters sit in cool water overnight after I did my second WFNA run. Seeing as it was winter and it's cold as all shit here in Maine, that was a big mistake. Came back in the morning to find my beautiful, delicate, ever-so-useful-but-not-anymore-because-f*ck-ice, distillation adapters... all caked in solid ice, broken into three pieces each. Needless to say, my reaction was similar to that of Tom Cruise's in "Rain Man". Except, replace the sand with snow.
https://www.youtube.com/watch?v=XRjoCb2a_nk


I did that once with a condenser, and decided never to let it happen again. Nothing has been destroyed yet, but I might get careless one day.




"Open your mind son, before someone opens it for you." - Dr. Walter Bishop
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3948
Registered: 8-2-2015
Member Is Offline


[*] posted on 29-1-2018 at 11:09


I too have had bad luck with 1l or more beakers,
(ok, I was careless) ... so far I've cracked

. a 1l hot horlicks mixer - pyrex
. a 1l cafetierre - toughened glass
. a 1.5l cafetierre - pyrex
. a 1l Griffin/low-form beaker - borosilicate

I had considered getting myself a nice Schott Duran 1l beaker
... untill I saw the cost. :o


largest undamaged beakers are now 250ml :P
so far I've not broken any beaker 250ml or less.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
PirateDocBrown
National Hazard
****




Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2018 at 11:39


Stainless steel beakers are available.



Phlogiston manufacturer/supplier.

For all your phlogiston needs.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2018 at 11:47


Quote: Originally posted by Deluxbert  
So i seem to be cursed because i have the great luck of constantly breaking 1000ml beakers. Just today I was drying up some iron oxide in a beaker and it just friggin popped. At 150C......


[Edited on 28-1-2018 by Deluxbert]


Were you using an oil bath or a sand bath?
View user's profile View All Posts By User
Reboot
Hazard to Others
***




Posts: 141
Registered: 8-8-2017
Member Is Offline

Mood: No Mood

[*] posted on 29-1-2018 at 12:46


Quote: Originally posted by Deluxbert  
I had it in my hands (wasnt even noticably warm) and it just cracked when I added some tap water for cleaning.


In many cases, 'breaking' from use is a drawn out process, with tiny fractures happening on many occasions for many reasons. Eventually the microscopic cracks accumulate and join up to become big cracks.

A glassblower once told me that thinner glass is more resistant to thermal stress since it's more flexible and heats more evenly (low thermal mass.) That may be, but it's more vulnerable to physical damage, which can make it more likely to be in a weakened state when it does come under thermal stress.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2324
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 30-1-2018 at 14:22


Ummm. I see the problem. A quick trip to e-bay, updated me on American/European Borosilicate prices. Not inexpensive anymore. In fact, the opposite of inexpensive prevails.

Gotta pick and peck, vintage labware, or go Chinese. Generally, even Vintage Pyrex costs a fortune.

Well, I'll log an e-bay watch-out, for desired items, and lay in wait.

[Edited on 30-1-2018 by zed]
View user's profile View All Posts By User

  Go To Top