Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Old decomposed Titanium (III) Chloride
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 4-6-2018 at 19:16
Old decomposed Titanium (III) Chloride


Hi all,

I recently bought an old (I'd estimate 30 years old) bottle of what was supposed to be a 20% solution of TiCl3. I didn't pay much and didn't expect too much. When it arrived, instead of a purple solution, there was a milky white suspension with considerable precipitate in the bottle - all of it yellowish white. The liquid is quite acidic - pH of about 1 to 0. The precipitate doesn't dissolve in an excess of water, nor in concentrated HCl, nor in about 50% H2SO4. Any idea what this gunk might be? The bottle cap was slightly loose when I received it (but wrapped with electrical tape) so I assume it was exposed to air for at least a few years. I think the solution was originally HCl in water with the TiCl3 also dissolved.

I was suspecting that the precipitate might be TiO2 but I thought that should dissolve in concentrated HCl.

It's difficult to find information about this chemical (TiCl3) because it seems that many sources confuse it with TiCl4, a super corrosive liquid which produces HCl fumes in air and reacts violently with water (I also have about 100mL of that from a previous acquisition so I am familiar with it).

Any info is appreciated!
Thanks,
Sean
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6454
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 4-6-2018 at 19:24


TiO2 sounds about right.
TiCl3 is not stable in aqueous solution and even in strong solutions of HCl it will hydrolyse over a matter of days if not hours.
OTOH, TiO2 is pretty impervious to HCl and will sit happily, doing nothing in the bottom of a container.




View user's profile View All Posts By User
sbreheny
Hazard to Others
***




Posts: 145
Registered: 30-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 4-6-2018 at 19:33


Quote: Originally posted by j_sum1  
TiO2 sounds about right.
TiCl3 is not stable in aqueous solution and even in strong solutions of HCl it will hydrolyse over a matter of days if not hours.
OTOH, TiO2 is pretty impervious to HCl and will sit happily, doing nothing in the bottom of a container.


Hmmm, well this was originally sold as a lab reagent so it must have had a shelf life of longer than days. I've attached a photo of the original label. This label just says "20% solution" but almost every other source I can find states that there is about 30% HCl in the solution rather than just water. Some of them also include phosphoric acid in about 3 to 5% concentration.

Can you think of any way to test whether this is indeed TiO2?

Sean


ticl3_sm.png - 406kB
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6454
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 4-6-2018 at 23:39


My experience with TiCl3 is from preparing it by reacting Ti powder with HCl. It won't have nearly the purity of proper reagent grade; it will have impurities, more exposure to oxygen and is likely to degrade a lot quicker.

AFAIK TiO2 is the stable form that titanium nearly always ends up as. I don't recall what hydroxides are possible, but really, what else could it be?

As for tests for TiO2, I am not sure there are any simple ones. Keen to know if someone does have one.

This probably means your reagent is ruined. TiO2 is really inert and not worth much.