flashpoint
Harmless
Posts: 16
Registered: 16-12-2003
Location: USA
Member Is Offline
Mood: No Mood
|
|
polyhydrocarbon plastic
How can I tell if plastic storage containers are made from polyhydrocarbon plastic?
Or better yet, do you guys know of any that aren't made of polyhydrocarbon?
I'm trying to store some MEKP for a short while, and can't find anything suitable for short time storage.
All I got in this world, is my balls and my word.
And I don\'t break em\' for nobody!
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
polyhydrocarbon? Do you mean polyolefin? Polystyrene is also a polyhydrocarbon, as it contains only C and H.
|
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
If you mean polyethylene, milk jugs are HDPE, as labeled. Many household products are HDPE, LDPE, polypropylene, polystyrene or PET (a polyester).
Tim
|
|
|
JohnWW
International Hazard
   
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
Polyethylene degrades in no time on exposure to the UV light in direct sunlight, unless it is filled with a black pigment.
|
|
|
flashpoint
Harmless
Posts: 16
Registered: 16-12-2003
Location: USA
Member Is Offline
Mood: No Mood
|
|
No, I mean Polyhydrocarbon, such as polyisobutylene, etc.
Have you ever put acetone on a piece of PVC piping? It softens it and melts it.
Thus why I wouldn't want to put any MEKP or wet ap into a polyhydrocarbon plastic. 
[Edited on by flashpoint]
All I got in this world, is my balls and my word.
And I don\'t break em\' for nobody!
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
| Quote: | Originally posted by flashpoint
No, I mean Polyhydrocarbon, such as polyisobutylene, etc.
...
[Edited on by flashpoint] |
http://en.wikipedia.org/wiki/Polyolefin
which however doesn't mention http://en.wikipedia.org/wiki/Butyl_rubber which is also a polyolefin, which because of the methyls sticking out form a soft rubbery material.
PVC is properly not a "Polyhydrocarbon" because of the chlorines, nor is nylon, PET and other polyesters, polycarbonate, acrylics, polysulfonones,
silicones, and so on.
About the only place the term "Polyhydrocarbon" shows up in regards to plastics is on patents and occasionally research papers. It is not commonly
used in the English speaking world as a term for plastics because it is too general, as I already said it covers the polyolefins/polyalkenes,
polystyrene, and several other uncommon plastics containing only carbon and hydrogen; it is just not a specific term.
If you mean "hydrocarbon" in the most general terms, ie 'organic', then almost all plastics are organic.
So, using terms common in the plastics industry, what is it you are after?
|
|
|
flashpoint
Harmless
Posts: 16
Registered: 16-12-2003
Location: USA
Member Is Offline
Mood: No Mood
|
|
I'm not sure now what I need.
I read throughout the posts I've read on MEKP not to store it in a polyhydrocarbon...so I'm guessing in any Poly's?
If you know how acetone softens/melts some plastics, but not others...this is why I suspect that it not be used to store MEKP, as it does the same to
plastics.
All I got in this world, is my balls and my word.
And I don\'t break em\' for nobody!
|
|
|
unionised
International Hazard
   
Posts: 4931
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
IIRC MEKP is usually stored as a mixture with something else for stabillity reasons. On of the things they use is dibutyl phthalate which is also used
as a plasticiser for PVC so I doubt that PVC would be suitable.
Have you tried searching for compatibility data for MEKP? Anyway, polypropylene, polyethylene, or PTFE are the most commonly used materials for
storing the stuff.
Oh, and BTW "Polyethylene degrades in no time on exposure to the UV light in direct sunlight, unless it is filled with a black pigment." is only going
to matter if you store ypour MEKP in direct sunlight and I really wouldn't advise doing that.
|
|
|
cool_arrow
Harmless
Posts: 15
Registered: 27-6-2005
Member Is Offline
Mood: No Mood
|
|
so why is a glass container not suitable?
|
|
|
sparkgap
International Hazard
   
Posts: 1234
Registered: 16-1-2005
Location: not where you think
Member Is Offline
Mood: chaotropic
|
|
^ as has oft been repeated, glass shrapnel is a terrible complication to have when your AP or MEKP suddenly decides not to play nice just because it
feels like it.
sparky (~_~)
"What's UTFSE? I keep hearing about it, but I can't be arsed to search for the answer..."
|
|
|