Author: Subject: Synthesis of polycarboxylic ether in lab.
bhupeshmulik
Harmless
*




Posts: 3
Registered: 4-3-2017
Member Is Offline

Mood: No Mood

[*] posted on 13-8-2018 at 02:43
Synthesis of polycarboxylic ether in lab.


hi,
can anyone explain the synthesis of MPEG based polycarboxylic ether in lab ?
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1744
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 14-8-2018 at 09:21


Not unless you explain more clearly what you mean by;

MPEG based polycarboxylic ether

PEG to me mean "polyethylene glycol" but the "M"?
View user's profile View All Posts By User
Waffles SS
Fighter
*****




Posts: 992
Registered: 7-12-2009
Member Is Offline


[*] posted on 14-8-2018 at 11:40


Quote: Originally posted by Boffis  
Not unless you explain more clearly what you mean by;

MPEG based polycarboxylic ether

PEG to me mean "polyethylene glycol" but the "M"?


MPEG is Methoxypolyethylene glycol.

For synthesis these type of polycarboxylic ether you need to make ester of this alcohol with Acrylic or Methacrylic acid and then do Co-Plomymerization with acrylic acid or Methacrylic acid.

Usally polycarboxylate use for concrete water reducer(Superplasticizer)


c3sm51030a-f1.gif - 6kB



There are many patent about synthesis of Polycarboxylate.just serach "mpeg polycarboxylate synthesis patent"



[Edited on 15-8-2018 by Waffles SS]