oxybate
Harmless
Posts: 38
Registered: 14-9-2006
Member Is Offline
Mood: No Mood
|
|
The Sodium Acetate Thing
Well I got a bunch of that.
However, it's not so easy as shown on YouTube. Anytime I try to cool the super-saturated solution I start to see crystallization - I'm wondering if
the dust in my condo is supplying the necessary seed matrix that is doing this. If that be the case, how can I achieve the fabled super-saturated
solution necessary to wow myself and my little cousins?
|
|
|
garage chemist
chemical wizard
   
Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline
Mood: No Mood
|
|
Do you cover the flask with some foil, and do you let it cool slow enough (only air cooling, no water)?
|
|
|
Jamjar
Harmless
Posts: 18
Registered: 2-7-2007
Member Is Offline
Mood: No Mood
|
|
Sodium acetate trihydrate loses water @ 120C.
Maybe the solution has dehydrated too much? Try adding a small amount of water <%10.
Impurities from vinegar?
Try cooling slower.
Sodium ethanoate ‘stalagmite’
|
|
|
UnintentionalChaos
International Hazard
   
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Cover when you cool, don't move it around, and cool it in a smooth walled (preferably new) glass container. Scratches on the glass can be enough to
make it crystallize. Keep any dust out of the mix.
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
|
oxybate
Harmless
Posts: 38
Registered: 14-9-2006
Member Is Offline
Mood: No Mood
|
|
Thanks for the suggestions. I followed the Youtube video which is quite deceptive.
|
|
|
16MillionEyes
Hazard to Others
 
Posts: 153
Registered: 11-3-2007
Location: 16 Million Eyes, US
Member Is Offline
Mood: No Mood
|
|
I've been wanting to do this myself but I don't have enough sodium acetate and I don't really have a way to measured how much I've produced and how
much I still need left. Also, I lost some yield trying to purify it the commonsense way (boil off) so I know rely on natural evaporation or cooling
filtration.
|
|
|