stoichiometric_steve
International Hazard
   
Posts: 818
Registered: 14-12-2005
Member Is Offline
Mood: satyric
|
|
spent Pd/C recycling/reactivation
this might have been discussed here, and i've actually had a procedure for this, but i've lost it and somehow, even trying TFSE didnt help. can
anybody help me out?
|
|
|
solo
International Hazard
   
Posts: 3883
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Here is a thread with the information you seek......solo
http://h1.ripway.com/solo/regeneratingPd-Ccatalyst.html
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
|
jon
National Hazard
  
Posts: 459
Registered: 11-1-2006
Member Is Offline
Mood: paranoid distrustful apprehensive
|
|
there was an article where they used basic solutions containing naoh to reactivate it.
a process operator i knew who is in the federal pen now told me they desulfurize gasoline with pd/c and the h2s poisons it so they reactivate it
using ammonia solutions so this is commonly done in industry too.
|
|
|
Klute
International Hazard
   
Posts: 1378
Registered: 18-10-2006
Location: France
Member Is Offline
Mood: No Mood
|
|
Exposing the spent catalyst to hydrogen would reactivate it, no? In that case, wouldn't adding a formate or other hydrogen donor in absence of a
acceptor produce hydrogen [1] and thus reactivate the catalyst? I think I remember something like that being mentionned at the Hive...
While on the subject, in the patent US4792625, they dry the reactivated catalyst with "a mixture of gases containing oxygen", which generates some
heat. What for?
Opening a bottle of nitrogen-flushed 10%Pd/C equally produces heat; does this diminish the quality of the catalyst if the protective atmosphere
isn't replaced quickly, and if the catalyst is used for a CTH and thus not directly exposed to hydrogen gas (which would supposebly strenghten it
again)?
[1] H.Wiener, Y,Sasson, J.Blum, J.Mol.Catal. 35, 27 (1986)
[Edited on 7-8-2007 by Klute]
|
|
|
jon
National Hazard
  
Posts: 459
Registered: 11-1-2006
Member Is Offline
Mood: paranoid distrustful apprehensive
|
|
you have to get all the poisons off the catalyst that's the pupose of using a basic solution. hydrogen would activate the catalyst so when you add
substrate the substrate does'nt poison or deactivate the catalyst.
|
|
|