Gallium and Field's metal alloy?!
Hello! What would happen if you alloy gallium metal with Field's Metal?
Would you get a liquid alloy with a lower melting point than the gallium indium tin alloy? Field's metal has bismuth in it.
So maybe it would make gallium indium tin bismuth alloy.
|
|
|
MrHomeScientist
International Hazard
   
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
I haven't been able to find a good table, but try searching low melting point alloys, fusible alloys, or eutectic alloys and you might find some
information. I imagine this would have a melting point between Galinstan and Field's metal. Try it and let us know!
|
|
|
fusso
International Hazard
   
Posts: 1907
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Quote: Originally posted by ChemistryGhost1  | Hello! What would happen if you alloy gallium metal with Field's Metal?
Would you get a liquid alloy with a lower melting point than the gallium indium tin alloy? Field's metal has bismuth in it.
So maybe it would make gallium indium tin bismuth alloy.
| Gallium is different from galinstan. Make sure you know the difference.
|
|
|
streety
Hazard to Others
 
Posts: 110
Registered: 14-5-2018
Member Is Offline
|
|
The eponymous Simon Quellen Field is very interested in science education and runs the sci-toys website. I don't think it answers your question exactly but he has pages discussing both the metal alloy he developed (i.e. Field's Metal) and the gallium, indium, and tin alloy that is liquid at room temperature
|
|
|