Pd/C vs. Pd/BaSO4


does anybody know if the difference on the solid support of Pd results in different activity or applicability for certain reductions? as far as specific area per gram matters, charcoal sure makes a difference vs. BaSO4.
View user's profile View All Posts By User
Klute
International Hazard
*****




Posts: 1378
Registered: 18-10-2006
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2008 at 06:02


It's not much, but in Chemical Reviews, (1985) 85(2), 129-170 they state:

" [the following] order of activity was found in the hydrogenolysis of benzyloxycarbonyl and benzyl protecting groups of peptides using cyclohexadiene as hydrogen donor, Ie., Pd black > 10%
Pd/C > 5% Pd/C > 10% Pd/BaS04 > 5% Pd/BaSO4."

ref provided: Felix, A. M.; Heimer, E. P.; Lambros, T. J.; Tzougraki, C.; Meienhofer, J. J. Org. Chem. 1978, 43, 4194.
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2008 at 09:26


Pd/BaSO4 will not reduce double bonds, but will reduce triple bonds, IIRC. It's basically Pd poisoned with Ba.



One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
solo
International Hazard
*****




Posts: 3967
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline

Mood: ....getting old and drowning in a sea of knowledge

[*] posted on 3-2-2008 at 09:31


.......see Rylander book on Hydrogenations there is lots of info there....solo



It's better to die on your feet, than live on your knees....Emiliano Zapata.
View user's profile View All Posts By User
Nicodem
Super Moderator
*******




Posts: 4230
Registered: 28-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 3-2-2008 at 13:16


Pd/BaSO4 is a slightly poisoned form of Pd catalyst that has some peculiar properties. For example, it can reduce acyl chlorides to aldehydes but not aldehydes to alcohols (not that Pd/C is particularly efficient at reducing aldehydes either, but Pd/BaSO4 does it more cleanly).
View user's profile View All Posts By User
WizardX
Hazard to Self
**




Posts: 61
Registered: 11-8-2005
Location: wizardx.4shared.com
Member Is Offline

Mood: wizardx.suddenlaunch3.com

[*] posted on 3-2-2008 at 15:10


PALLADIUM CATALYSTS http://www.orgsyn.org/orgsyn/prep.asp?prep=cv3p0685



Albert Einstein - \"Great ideas often receive violent opposition from mediocre minds.\"
View user's profile Visit user's homepage View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 3-2-2008 at 18:28


Quote:
Originally posted by Klute
It's not much, but in Chemical Reviews, (1985) 85(2), 129-170 they state:

" [the following] order of activity was found in the hydrogenolysis of benzyloxycarbonyl and benzyl protecting groups of peptides using cyclohexadiene as hydrogen donor, Ie., Pd black > 10%
Pd/C > 5% Pd/C > 10% Pd/BaS04 > 5% Pd/BaSO4."

ref provided: Felix, A. M.; Heimer, E. P.; Lambros, T. J.; Tzougraki, C.; Meienhofer, J. J. Org. Chem. 1978, 43, 4194.


I don't quite see the applicability of this paper but here it is:

Attachment: jo00415a045.pdf (371kB)
This file has been downloaded 1754 times





"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)