Substitute high boiling point solvent
The literature says to use trichlorobenzene and bring the temperature to over 200*C and then filter and wash the product with benzene. Since TCB is a
hazardous material, I'd like to use a different (cheap?) aprotic non-polar solvent with a similar boiling point. Any suggestions?
Thanks!
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Depends on the reactants different solvents may or may not be compatible with the reagents and products.
|
|
Nicodem
|
Thread Moved 1-9-2011 at 07:50 |
exciton
Harmless
Posts: 3
Registered: 31-8-2011
Member Is Offline
Mood: No Mood
|
|
Reagents are: pyromellitic dianhydride and urea. The product will be poly-phthalocyanine.
Any suggestions?
|
|
exciton
Harmless
Posts: 3
Registered: 31-8-2011
Member Is Offline
Mood: No Mood
|
|
Okay, so I figured out that the _test tube_ containing pyromellitic dianhydride and urea is placed in a high boiling point solvent (such as
dipropylene glycol) but the contents _in_ the test tube are not solvated by them. In other words, if I understand this correctly, the reactants
remain dry.
I'll eventually give it a try. I'm excited to see if I can produce a cheap organic polymer solar cell from a poly-phthalocyanine dye precursor. ![:)](./images/smilies/smile.gif)
|
|
fledarmus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 187
Registered: 23-6-2011
Member Is Offline
Mood: No Mood
|
|
Then you're just using the trichlorobenzene as a heating bath?
For 200*C, I think I would switch to a sand bath. That's a little high for the mineral oil baths I would otherwise suggest, and high-temp silicon oil
is pretty pricey.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
You could try diphenyl ether; widely used for ring closures, decarboxylations, etc.
|
|