Melting tellurium powder


I have some tellurium powder, and I was hoping to melt a couple grams of it into a little ingot (or at least a blob) to have as an element sample. I searched the forum, but couldn't find any information about melting tellurium. I assume either inert gas or a flux of some kind will be needed to prevent oxidation.

Due to its relatively low melting point, I thought perhaps I could put the powder into a borosilicate glass ampoule, purge with inert gas, and seal it. Then I could heat the entire ampoule above the melting point of Te, which is still well below the softening point for borosilicate. Has anyone tried something like this before?

[Edited on 12-11-2023 by Texium]




Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6238
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 11-12-2023 at 16:13


I would be hesitant to heat a sealed ampoule. Gas expansion could ruin your sample.

Easier to neck a test tube, melt the Te with an argon flow, then seal.
Or, if it is just for an element sample, I have a nice crystalline piece Zi could give you.
(I can't really see that I will get into Te chemistry.)
View user's profile View All Posts By User
Admagistr
Hazard to Others
***




Posts: 350
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 11-12-2023 at 16:33


A friend who sells chemical elements melts selenium powder regularly to get nice samples to sell and does it in the air!Of course he covers the crucible with a sealing lid.I think he uses a corundum crucible. But he complains,even when he does the work outdoors and with a mask,that he always smells a bit of selenium,he likens it to a sulphur-like smell.He has a degree and exam in toxicology and knows the dangers of selenium compounds.If you want to try it,I can ask him for details,tellur is selenium-like,so it should work similarly...
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 16-12-2023 at 12:46


Goodness gracious, you couldn't pay me enough to melt Se or Te in air!



Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
Admagistr
Hazard to Others
***




Posts: 350
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 16-12-2023 at 14:15


Quote: Originally posted by Fleaker  
Goodness gracious, you couldn't pay me enough to melt Se or Te in air!


I've also heard about thallium smelting and the emerald flame that appeared during it, but the details were withheld from me, that they don't talk about such things...I would never go for it either, but there is always someone who knows that they will make a very good profit and do it:(That's life...