Thank you for such detailed information and pictures. I agree on the pursuit of the most powerful det cap is a waste of time. Its sol purpose is to
initiate the secondary. Just add a booster if you want a stronger initiation. It’s hard to follow up with a response to the fine work you’ve
done.
|
|
Laboratory of Liptakov
International Hazard
Posts: 1342
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: cool.gif
|
|
Thanks. Basic detonator must penetrate 2 mm construction steel at 300mg ETN and 3 mm plate at 500mg ETN. Thats enough good for next
steps as is booster or using of else secondary EM. Nothing big science....