Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Rice husk ash, an amazing material and its uses!
rockyit98
Hazard to Others
***




Posts: 246
Registered: 12-4-2019
Location: The Known Universe
Member Is Online

Mood: no mood is a good mood

[*] posted on 12-1-2021 at 04:44
Rice husk ash, an amazing material and its uses!


rice being the most harvested crop we are left with agricultural waste such as
Rice husk in vast quantities .https://en.wikipedia.org/wiki/Rice_hulls with in it 20% of its dry mass is SiO2. after full burn it's concentrated up to 95% by mass of the ash which is pure white but left over carbon can make black or grey . it can be use to make insulation material up to 1300C as it is, and just mixing with slacked lime(Ca(OH)2) can make Calcium-silicate bricks and sheets for refractory. if you heat Rice hulls in a microwave with proper insulation (1500C) can make SiC micro particles. the ash can be used to make Na2SiO3 with ease. rice hull charcoal can be used in the production of elemental phosphorus.




MMH- You sure this thing won't blow up?
Silas- it won't blow up. But I can't guarantee it won't implode.
View user's profile View All Posts By User
TriiodideFrog
Hazard to Others
***




Posts: 107
Registered: 27-9-2020
Member Is Offline


[*] posted on 12-1-2021 at 04:53


Interesting. Could you further explain on the phosphorus part?
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 246
Registered: 12-4-2019
Location: The Known Universe
Member Is Online

Mood: no mood is a good mood

[*] posted on 12-1-2021 at 05:19


Quote: Originally posted by TriiodideFrog  
Interesting. Could you further explain on the phosphorus part?

4 Ca5(PO4)3F + 18 SiO2 + 30 C → 3 P4 + 30 CO + 18 CaSiO3 + 2 CaF2

SiO2 and C are from R.H.A and rice hull charcoal.




MMH- You sure this thing won't blow up?
Silas- it won't blow up. But I can't guarantee it won't implode.
View user's profile View All Posts By User
njl
International Hazard
*****




Posts: 520
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 12-1-2021 at 07:14


If rice husks are 20 percent silica by dry mass, how can they be turned into effective charcoal? Isn't the purpose of charcoal to get relatively pure carbon?
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 246
Registered: 12-4-2019
Location: The Known Universe
Member Is Online

Mood: no mood is a good mood

[*] posted on 12-1-2021 at 11:37


Quote: Originally posted by njl  
If rice husks are 20 percent silica by dry mass, how can they be turned into effective charcoal? Isn't the purpose of charcoal to get relatively pure carbon?

it's depend on the use case , if you need to make SiC having SiO2 is an advantage because its fine and well mixed .half of work done for you.




MMH- You sure this thing won't blow up?
Silas- it won't blow up. But I can't guarantee it won't implode.
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1883
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 13-1-2021 at 11:23


How does SiO2 get into the rice husk in the first place? As soluble silicate salts?
View user's profile View All Posts By User
RustyShackleford
Hazard to Others
***




Posts: 128
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline


[*] posted on 13-1-2021 at 11:45


Quote: Originally posted by fusso  
How does SiO2 get into the rice husk in the first place? As soluble silicate salts?

In the ocean i think the main method species aborb SiO2 is by conversion to H4SiO4, might be the same for rice
View user's profile View All Posts By User
karlos³
International Hazard
*****




Posts: 1115
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: verrückt & wissenschaftlich

[*] posted on 14-1-2021 at 07:15


Reminds me of the fly ash as catalyst sort of papers?
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 246
Registered: 12-4-2019
Location: The Known Universe
Member Is Online

Mood: no mood is a good mood

[*] posted on 14-1-2021 at 14:29


Quote: Originally posted by fusso  
How does SiO2 get into the rice husk in the first place? As soluble silicate salts?
\
nobody knows for sure (at least I think). further research is needed.




MMH- You sure this thing won't blow up?
Silas- it won't blow up. But I can't guarantee it won't implode.
View user's profile View All Posts By User
EthidiumBromide
Harmless
*




Posts: 42
Registered: 27-9-2020
Member Is Offline

Mood: Effervescent

[*] posted on 15-1-2021 at 05:19


It has been partially elucidated, rice in particular has an aquaporin-type membrane protein of the NIP2 family, primarily expressed in roots, which is responsible for uptake of Si in the form of Si(OH)4.
https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2048782/pdf/pp1...

Some other plants also have related NIP2 aquaporins that can transport Si(OH)4. https://sci-hub.do/10.1007/s11103-013-0087-3
View user's profile View All Posts By User
rockyit98
Hazard to Others
***




Posts: 246
Registered: 12-4-2019
Location: The Known Universe
Member Is Online

Mood: no mood is a good mood

[*] posted on 15-1-2021 at 05:25


https://www.youtube.com/watch?v=6KU1HrM67Ms

Two U-M researchers turn useless waste from rice processing into the high-purity silica compounds that are used in everything from toothpaste to tires. The technique could eliminate millions of tons of CO2 emissions every year, and it’s 90 percent less expensive than the
current method




MMH- You sure this thing won't blow up?
Silas- it won't blow up. But I can't guarantee it won't implode.
View user's profile View All Posts By User