| Search |
| [Next Page] |
Homemade capacitor for a power supply In a word, no.
Commercial electrolytic capacitors have a number of advantages which would be hard ... |
4-8-2010 at 07:30 by: densest |
Removal of Oxygen & Carbon Dioxide from Air (Glovebox Design) @aliced25 - from what you're saying, it sounds like you're not in the USA. Can you buy liquid nitrog ... |
1-8-2010 at 06:29 by: densest |
Removal of Oxygen & Carbon Dioxide from Air (Glovebox Design) That's all plausible. Consider it as an engineering question:
What's more fun and more important ... |
31-7-2010 at 23:43 by: densest |
Removal of Oxygen & Carbon Dioxide from Air (Glovebox Design) Depending on where you live, it may be cheaper to buy nitrogen or argon from a welding supply house. ... |
31-7-2010 at 20:13 by: densest |
Electrolytic DEplating of silver from copper? The I2/KI method is interesting. Of course, buying iodine is impossible in the US without DEA paperw ... |
31-7-2010 at 11:19 by: densest |
fume hood design I gave it above - cfm of fan / ( 60 * area of opening in square feet)
|
30-7-2010 at 19:05 by: densest |
Magnesium powder from magnesium pencil sharpener Uhhhhhhhhh.... Read Lloyd Sponenburgh's book on ball milling. At the end, he gives a very chilling s ... |
30-7-2010 at 18:55 by: densest |
fume hood design That one looks good. Do the math for your hood - I use an arbitrary value of 1 foot per second of ai ... |
30-7-2010 at 18:50 by: densest |
fume hood design I wouldn't use it - the motor is inside the air stream. I've had to replace such a fan twice in the ... |
30-7-2010 at 18:46 by: densest |
fume hood design @bob800 - the blower you referenced will not push against an air filter. If you release corrosive or ... |
30-7-2010 at 18:36 by: densest |
fume hood design Blowers like the one pictured a few posts above are perfectly suitable for a fume hood. The motor is ... |
30-7-2010 at 18:28 by: densest |
fume hood design The jewelry maker's hood would probably be OK for HOLDING COLD INORGANIC fumes. It would be hazardou ... |
30-7-2010 at 11:34 by: densest |
Electrolytic DEplating of silver from copper? @goldsilverpro - are there similar solutions for removing gold from copper? I'm trying to avoid cyan ... |
30-7-2010 at 11:24 by: densest |
fume hood design Flammable plastics, heat, and solvents -> splattered flaming plastic stuck to your flesh. A very ... |
29-7-2010 at 09:09 by: densest |
Potassium metabisulfite to K2CO3 or KOH Another name for potassium carbonate is "pearl ash" which is available at potter's supply stores.
... |
28-7-2010 at 16:40 by: densest |
Iodine from seaweed It's probably not practical... some beaches get covered with smelly decomposing seaweed & it's s ... |
28-7-2010 at 14:33 by: densest |
Starting a small buissness? If what you want to do is make scents, check out www.libertynatural.com who sell hundreds of oils, e ... |
28-7-2010 at 14:28 by: densest |
Potassium metabisulfite to K2CO3 or KOH KCl is often sold as potassium-only fertilizer. Since plants absolutely require potassium, you must ... |
26-7-2010 at 13:55 by: densest |
DIY Flashback Arrestor How much H2 and total gas are you thinking about? I have a 150 mL/min H2 generator. Connecting it to ... |
26-7-2010 at 12:14 by: densest |
Cleaning Glassware W/Acid-base Washes The sodium/sulfur/oxygen compounds sold for removing rust (hydro/pyro/sub/poly/meta/???/sulfite - ch ... |
21-7-2010 at 13:40 by: densest |
troubleshooting a homemade hotplate Oooooh! Must have Thanks!
The same person is selling 1500W stovetop heating elements for $15 ... |
21-7-2010 at 13:27 by: densest |
troubleshooting a homemade hotplate @peach - Thanks, yes, there are bad days and bad weeks... sometimes bad years.
Agreed, yes, the b ... |
20-7-2010 at 22:34 by: densest |
Cleaning Glassware W/Acid-base Washes As usual... it depends. What's on the glassware? Organics? Food products? Tars? You really want surf ... |
20-7-2010 at 21:44 by: densest |
DIY Flashback Arrestor Back in the glory .05 days of cold fusion, catalytic recombination modules intended for sealed lead- ... |
20-7-2010 at 21:32 by: densest |
DIY Flashback Arrestor Standard welding arrestors work fine with H2, AFAIK. Probably cheaper than a condenser & distill ... |
20-7-2010 at 10:43 by: densest |
| [Next Page] |