Search |
iron gall ink Looks great! If you're adding acacia, you probably won't want to use the ink in a fountain pen. I' ... |
9-8-2014 at 19:16 by: fiberdrunk |
iron gall ink Here are the same samples 24 hours later:
[img]https://farm6.staticflickr.com/5560/14699214521_12 ... |
20-7-2014 at 13:00 by: fiberdrunk |
iron gall ink [rquote=339011&tid=31203&author=Artemus Gordon]Very pretty pictures, Fiberdrunk!
Is the b ... |
20-7-2014 at 11:27 by: fiberdrunk |
iron gall ink [rquote=338984&tid=31203&author=Fenir]How well does the ink adhere to the paper? Could you s ... |
19-7-2014 at 17:17 by: fiberdrunk |
iron gall ink [rquote=338975&tid=31203&author=aga]Brilliant ![/rquote]
Thanks!
Here's another samp ... |
19-7-2014 at 12:41 by: fiberdrunk |
iron gall ink I wanted to test out how this ink shades. I wrote these samples on Strathmore 100% Cotton using a 3 ... |
19-7-2014 at 12:06 by: fiberdrunk |
Ink is Finished! I made the ink! Here is a photo of the ink used in different fountain pens and a glass dip pen.
... |
15-7-2014 at 07:57 by: fiberdrunk |
New Research on Iron Gall Ink I found an interesting 2 1/2 hour video on YouTube by the Library of Congress: [url=https://www.you ... |
11-7-2014 at 17:43 by: fiberdrunk |
iron gall ink [rquote=337732&tid=31203&author=zts16]Ok thanks, I'll do that. Hopefully I won't get nasty w ... |
9-7-2014 at 16:20 by: fiberdrunk |
iron gall ink [rquote=337723&tid=31203&author=zts16]Ok, so I'm getting a little bit concerned, because I h ... |
9-7-2014 at 14:11 by: fiberdrunk |
iron gall ink [rquote=337693&tid=31203&author=aga]Fascinating.
"boil it covered for 10 minutes to kill ... |
9-7-2014 at 11:23 by: fiberdrunk |
iron gall ink [rquote=337685&tid=31203&author=aga]Cool !
Making is Definitely much more fun than just Bu ... |
9-7-2014 at 10:59 by: fiberdrunk |
iron gall ink [rquote=337422&tid=31203&author=Artemus Gordon][rquote=336988&tid=31203&author=fiber ... |
9-7-2014 at 09:16 by: fiberdrunk |
iron gall ink [rquote=337278&tid=31203&author=aga][rquote=337204&tid=31203&author=Pinkhippo11]Are ... |
9-7-2014 at 08:57 by: fiberdrunk |
iron gall ink Your ink turned out really nice! |
6-7-2014 at 12:58 by: fiberdrunk |
iron gall ink [rquote=336989&tid=31203&author=No Tears Only Dreams Now]If you're already going to have som ... |
4-7-2014 at 13:36 by: fiberdrunk |
iron gall ink [rquote=336939&tid=31203&author=Pinkhippo11]Recently for a history project I synthesized two ... |
4-7-2014 at 05:30 by: fiberdrunk |
iron gall ink [rquote=336918&tid=31203&author=Artemus Gordon]I found this in the Wikipedia entry for Iron ... |
4-7-2014 at 04:44 by: fiberdrunk |
iron gall ink [rquote=336893&tid=31203&author=Artemus Gordon]
My pleasure, and please do post any exper ... |
3-7-2014 at 12:41 by: fiberdrunk |
iron gall ink [rquote=336848&tid=31203&author=Artemus Gordon]Fiberdrunk, all those chemicals can be ordere ... |
3-7-2014 at 05:18 by: fiberdrunk |
iron gall ink [rquote=336780&tid=31203&author=zts16]Ok, cool, that's great! And the links are very helpful ... |
2-7-2014 at 08:31 by: fiberdrunk |
iron gall ink [rquote=336774&tid=31203&author=zts16]Traditionally, as the name suggests, iron gall ink was ... |
2-7-2014 at 07:49 by: fiberdrunk |
iron gall ink [rquote=336769&tid=31203&author=Cheddite Cheese]Sulfuric acid is sold as Rooto drain cleaner ... |
2-7-2014 at 07:42 by: fiberdrunk |
iron gall ink This is my first post. I was referred here by a [url=http://www.fountainpennetwork.com/forum/]Fount ... |
2-7-2014 at 07:01 by: fiberdrunk |