| Search |
| [Next Page] |
The amount of primary needed Don't use that amount with a cap using RDX as the base charge though. SADS is weaker than LA or MF. |
18-11-2013 at 16:43 by: golfpro |
The amount of primary needed 250mg pressed |
18-11-2013 at 07:14 by: golfpro |
Performance of "Damp" AN As for the density not sure, I don't have the tools to accurately measure, but I do know that presse ... |
17-11-2013 at 07:42 by: golfpro |
Performance of "Damp" AN Why PBX ETN? Well the binder brings the density up to around 1.5g/ml that can not be had by pressing ... |
16-11-2013 at 09:49 by: golfpro |
Performance of "Damp" AN Hi,
It can be a difficult task to keep AN dry even in prill form, but if left in a semi-sealed ... |
16-11-2013 at 07:50 by: golfpro |
Erythritol powdered or coarse (ETN) This can be used, I've done it this one says to allow the ETN to rise up to 40*C and then keep it at ... |
11-11-2013 at 14:31 by: golfpro |
Erythritol powdered or coarse (ETN) I have made ETN multiple times before and I've always got around the same amount of Erythritol Tetra ... |
10-11-2013 at 14:19 by: golfpro |
erythritol tetranitrate recrystallization I've been experimenting a bit (had some free time today) with a different way of making ETN using an ... |
10-11-2013 at 12:50 by: golfpro |
Hobbyist lab setup You should be OK w/ those, watch out for nitric acid though in large amounts |
30-10-2013 at 17:45 by: golfpro |
Det Cord w/ ETN Has anyone tried making a det. cord using ETN as the core? What kind of tubing? I was thinking filli ... |
28-10-2013 at 17:59 by: golfpro |
About toxicity of explosives What????? Just don't eat ETN and you'll be OK. Even if you do eat a little bit, you will just get a ... |
27-10-2013 at 14:40 by: golfpro |
How to neutralize TATP You'll get .01 grams of TATP from that low concentration hydrogen peroxide. |
25-10-2013 at 13:46 by: golfpro |
Is this a method for Cocrystalization 100g ETN and 20g RDX. This is the approximate formula for a perfect oxygen balance between the two. |
24-10-2013 at 16:00 by: golfpro |
ETN synthesis issue stirring with a glass rod is annoying and takes a lot of effort. I am also looking for a replacement ... |
24-10-2013 at 15:58 by: golfpro |
Critical diameter You can watch Ral's video on youtube, cast bit of ETN doesn't detonate in a straw even when subject ... |
24-10-2013 at 14:15 by: golfpro |
Is this a method for Cocrystalization Say we have 100g of material A and 20g of material B both of these are soluble in Acetone although M ... |
24-10-2013 at 14:13 by: golfpro |
golfpro's Nitric Acid for Beginners I hate ordering chemicals online but I might have to. I read about using ammonium nitrate for this a ... |
23-10-2013 at 18:14 by: golfpro |
NaNO3 instead of KNO3 for nitric acid distillation Hi,
I have lost my source of KNO3 which I distilled from H2SO4 to produce HNO3, I may no longer ... |
23-10-2013 at 17:47 by: golfpro |
Nitroguanidine wikipedia says anywhere from 7400-8100 depending on which page you look at.
I wish there was an o ... |
22-10-2013 at 15:56 by: golfpro |
Nitroguanidine If it's true density is 1.7 than that would be good, but it has a low heat of explosion, I don't see ... |
21-10-2013 at 17:54 by: golfpro |
Nitroguanidine "Nitroguanidine has a VoD of 8200 m/s at density of 1.70 g/cm3"
Who says this?? wikipedia gives ... |
20-10-2013 at 17:49 by: golfpro |
More usefull explosives when making RDX It can be synthesized, anything can be if you want it bad enough and are willing to put in the time ... |
18-10-2013 at 17:07 by: golfpro |
Dense AN prills, booster needed? [rquote=303704&tid=26743&author=hyfalcon]95% AN with 5% 5 micron Al will detonate from anyth ... |
17-10-2013 at 12:07 by: golfpro |
Dense AN prills, booster needed? I figure that with enough booster and with the material fully evenly mixed (the prills are coated wi ... |
17-10-2013 at 11:11 by: golfpro |
Dense AN prills, booster needed? I have AN in the form of tiny prills, these are dense, I like the idea of keeping them prills becaus ... |
16-10-2013 at 16:10 by: golfpro |
| [Next Page] |