References on Downs' Cell Design/Construction I have been tempted to make one at several different times in the past as my metalworking skills imp ... |
27-3-2024 at 21:02 by: markgollum |
Comfort level with dimethyl sulfate No, I would not work with dimethylsulfate while expecting to be protected by outdoor ventilation.
I ... |
26-9-2022 at 11:13 by: markgollum |
Somewhat Unusual Properties of Ammonium Benzoate Ammonium benzoate is quite an effective corrosion inhibitor for ferrous metals. It is used commercia ... |
29-3-2022 at 14:25 by: markgollum |
Batteries are Friggin Complicated Yo (also voltage determination) I would say that because open circuit voltage is a thermodynamic property of the system, that the va ... |
29-9-2020 at 20:44 by: markgollum |
Dimethyl oxalate synthesis problems I made dimethyl oxalate many years ago, I did it a number of times but never got a great yield, I r ... |
18-7-2020 at 02:22 by: markgollum |
Check your U2U |
29-8-2012 at 17:22 by: markgollum |
A Salute to Sir Frank MacFarlane Burnett Well, one pest that I really could see somebody exterminating with biological warfare is the pine be ... |
26-1-2011 at 19:10 by: markgollum |
picramic acid from picric I would actually prefer to directly reduce sodium sulfate for the following reasons.
1) After ext ... |
24-1-2011 at 21:10 by: markgollum |
picramic acid from picric I have been reading about all the many things that people have been trying and proposing to get picr ... |
24-1-2011 at 09:54 by: markgollum |
Passivation of MMO anode? @ dann2
Yes, I would agree that 2 cathodes are better than one.
@woelen
I would also agree w ... |
10-1-2011 at 20:42 by: markgollum |
Passivation of MMO anode? Sorry for the multiple post
[file]12668[/file] |
9-1-2011 at 14:14 by: markgollum |
Passivation of MMO anode?
[file]12666[/file] |
9-1-2011 at 14:10 by: markgollum |
I have had a similar experience I have had two MMO anodes passivate/wreck on me. This was a good 3 years back so my memory is slight ... |
9-1-2011 at 14:05 by: markgollum |
Thermocouples I have a nice type K thermocouple probe in an a nickel superalloy sheath (not sure which super alloy ... |
11-6-2009 at 19:51 by: markgollum |
Purification of Spongy Alloy When I fused CaCl2 to use as a dessicant, I was surprised just how volatile it was. I think you shou ... |
25-5-2009 at 18:12 by: markgollum |
Fuel-Air Explosives If you are wondering if one metal or other fuel can "strip" the oxygen from another, an Ellingham di ... |
11-5-2009 at 16:09 by: markgollum |
Zinc in brass does not react with acids? The galvanic series is valid even on the atomic scale. But interestingly, there are many galvanic se ... |
6-4-2009 at 16:54 by: markgollum |
Calcium Sulphide I have reduced calcium sulphate to the sulphide twice. I did it by grinding together the CaSO4 + cha ... |
9-3-2009 at 20:01 by: markgollum |
Sulphur Trioxide and Oleum Using a Box Oven - Illustarted Practical Guide SUPERB WORK!!
I am again impressed with the quality and usefulness of your practical guide.
I ... |
13-4-2008 at 21:40 by: markgollum |
Looking For Amyl Alcohol (x-pentanol) Source I would agree with woelen and contrabasso on this subject.
If you are not very well equipped to saf ... |
12-4-2008 at 10:34 by: markgollum |
KCLO3 by way of H2O + KCL @ dann2
In reply to your question, I don't know for certain what the MMO anode I have is specifical ... |
11-4-2008 at 16:08 by: markgollum |
More on PbO2 electrodes I have a nice chlorate cell using a MMO anode and Ti cathode but in my design the electrodes are bol ... |
4-4-2008 at 21:51 by: markgollum |
Solid Phase Reaction Vessel? Guess what, I was also thinking about buying one of them!! 
And no, I don't know what they are us ... |
25-3-2008 at 20:11 by: markgollum |
Trinitrotoluene preparation To Bonome and others who believe they have made TNT:
How do you know that what you have is in fact ... |
1-3-2008 at 15:31 by: markgollum |
Platinum plated titanium I found a supplier on Ebay that sells platinised titanium anodes as well as MMO Ti anodes.
http:/ ... |
2-2-2008 at 18:31 by: markgollum |