Search |
Obtaining Hexane (Down-under) Beware that commercial hexane has heavy ends in it.
There is a company that uses it for extractio ... |
16-11-2010 at 06:18 by: morrie |
Cerium Oxide I have kilo of nano cerium oxide. I have had it for years. Not much use for anything that I can th ... |
16-11-2010 at 06:07 by: morrie |
Hello to the forum I could not find any welcome sticky anywhere, so I am using this thread to say hello. I have had a ... |
16-11-2010 at 05:24 by: morrie |
Red mud in Donau in Hungary what is it ? I worked for 20 years in the bauxite alumina industry.
Red mud is alkaline!! No doubt about it. ... |
16-11-2010 at 05:11 by: morrie |
filtering a Zinc Chloride solution I used to run a plant where we used zinc chloride as a feed material to our process. We purchased i ... |
16-11-2010 at 05:02 by: morrie |