A water resistant hot glue from expired milk proteins Hello fellow chemists,
in this experiment I present the preparation of a strong, water-proof, hot ... |
16-1-2026 at 19:57 by: palico |
6- Benzyl Azulene synthesis Dear Ormarion,
well done, nice job ! I confess, your lab quite scare me...
Anyway, your azul ... |
16-1-2026 at 19:02 by: palico |
Glassware For Sale from previous Organic Chemistry/Biotechnology laboratory (!) Updates progressively I am interested in many of those items, but I do not understand if price is per unit of for the whol ... |
12-1-2026 at 01:50 by: palico |
A black ink and fabric dyes from spent coffee pods Yes, it is very cool. I recommendo to try this experiment, even with other waste biomass. |
10-1-2026 at 17:07 by: palico |
Amateur Chemistry in Australia Dear InFormation,
welcome to this forum. I have no idea about australian regulations, but in plac ... |
9-1-2026 at 13:45 by: palico |
A black ink and fabric dyes from spent coffee pods Hello fellow chemists,
I back from a long pause of my activity on this forum. Today I present you ... |
9-1-2026 at 13:39 by: palico |
Binaphthyl and perylene My advice is to do a literature research on the Scholl reaction. There should be a modern reagent to ... |
9-1-2026 at 12:47 by: palico |
Cheapest Source of Chlorine The cheapest and more available source to generate chlorine gas, are the one you mentioned in the be ... |
19-11-2024 at 12:53 by: palico |
Chemical Liquidation - Elemental Scientific Do you ship to EU ? |
3-10-2024 at 13:40 by: palico |
Synthesis of benzene from PET water bottles [rquote=693316&tid=160130&author=Mateo_swe]Are this just for an intresting method of doing s ... |
8-7-2024 at 13:13 by: palico |
Synthesis of benzene from PET water bottles I have no idea about application of vacuumin pyrolysis, it helps instead nitrogen flushing before re ... |
14-5-2024 at 15:49 by: palico |
Synthesis of benzene from PET water bottles [rquote=692215&tid=160130&author=dettoo456]Moved from other thread:
This paper (https:// ... |
25-4-2024 at 07:56 by: palico |
Synthesis of terephthalic acid from a PET water bottle [rquote=692323&tid=160150&author=Hexabromobenzene]Terephalic acid is of little interest. In ... |
9-4-2024 at 20:22 by: palico |
Synthesis of terephthalic acid from a PET water bottle Dear detto:
indeed, by pyrolysis of PET it is possible to get benzene directly. I performed this ... |
3-4-2024 at 21:30 by: palico |
Synthesis of quinizarin Hello. Wonderful synthesis and product. The product of first crystallization has the same color of a ... |
3-4-2024 at 10:44 by: palico |
Two-step preparation of biodiesel from waste soap Dear bnull, as solution I offered to distill of any volatiles before extracting residual fatty acids ... |
1-4-2024 at 13:57 by: palico |
Two-step preparation of biodiesel from waste soap Dear bnull, yes transesterification of ethyl acetate is a possible solution, it is discussed in my r ... |
28-3-2024 at 04:51 by: palico |
Two-step preparation of biodiesel from waste soap Hello people !
here another episode of the waste to resource experiment list: today we see the pr ... |
27-3-2024 at 16:04 by: palico |
Synthesis of Mesitylene I would like to perform that reaction. Technically is a cyclodehydration, so other dehydrating agent ... |
27-3-2024 at 14:56 by: palico |
Synthesis of terephthalic acid from a PET water bottle dear dicyanin, i see you are a great chemical experimentalist. I do not so much on your TLC plate, t ... |
27-3-2024 at 14:50 by: palico |
Synthesis of terephthalic acid from a PET water bottle Dear dicyanin, thanks for your experiment, but how have you checked the identity and purity of your ... |
25-3-2024 at 07:27 by: palico |
Synthesis of fatty acids from expired soap Your considerations are all correct. |
14-3-2024 at 06:48 by: palico |
Synthesis of fatty acids from expired soap @chornedsnorkack: I have no idea which one those degradation reaction has occurred to my soap.
@c ... |
13-3-2024 at 08:12 by: palico |
Synthesis of fatty acids from expired soap Hello people !
today another episode of the waste to resource series. I am thinking to rename it ... |
13-3-2024 at 03:58 by: palico |
Preparation of biodiesel from waste cooking oil Hello Dr. Bob. To know if that biodiesel is good for trasportation it requires more accurate analysi ... |
6-3-2024 at 02:42 by: palico |
| [Next Page] |