stannous chloride Thanks for suggestions people. Woelen's suggestion did the trick. I added a 3% solution of Hydrogen ... |
6-12-2016 at 12:18 by: palladiumdreams |
stannous chloride I figured I had "purple of Cassius" but I did not think silver (nitrate) would cause that effect.. T ... |
29-11-2016 at 02:46 by: palladiumdreams |
stannous chloride The color is brilliant purple like permanganate.
Very sure it is not titanium, the Tin melted on lo ... |
28-11-2016 at 12:34 by: palladiumdreams |
stannous chloride Glassware was clean with no traces of precious metals or permanganates present. I checked the tin an ... |
25-11-2016 at 18:25 by: palladiumdreams |
stannous chloride I am trying make a 2M solution of stannous chloride and am getting left with a purple solution once ... |
25-11-2016 at 01:33 by: palladiumdreams |