My 2 neck flask is broken :(

vmelkon - 18-11-2018 at 09:45

I was trying to distill some impure H2SO4 and this requires high temperature, even when I reduced the pressure to 13 cm mercury.

It was a 2 neck flask.
I had placed a solid glass stopper in one of the necks. I guess it expanded and cracked the neck :(

My glassware is broken and my heart is broken :(

Ubya - 18-11-2018 at 09:50

i would be scared more of the hot boiling sulphuric acid spilling than sad for the lost of a flask

nimgoldman - 18-11-2018 at 11:55

I feel for you.

I have melted one 3-neck flask when drying molecular sieves under vacuum using a heating mantle.

After several pieces of broken glassware, I think about purchasing the cheaper kinds (flasks, beaker) in quantity as they have limited life expectancy in every lab.

VSEPR_VOID - 18-11-2018 at 16:08

Press F to pay respects to the flask

Dragonjack12 - 3-12-2018 at 12:06

F

unionised - 3-12-2018 at 12:30

https://www.youtube.com/watch?v=D05AB8xs7qA

morganbw - 3-12-2018 at 12:46

I basically love my glassware but life has chosen to show me that it can be broken. Start some lab work that requires this/a certain piece and the damn thing is sure to break. I just figured it was me and my karma.