John paul III - 14-3-2019 at 17:37

I was wondering what is the nitrogen content of the flash paper marketed as a tricksters item. It seems to leave no residue upon combustion but that's not a good indication of the degree of nitration. Has anyone here compared high quality homemade nc with this stuff or could otherwise share some knowledge?

MineMan - 15-3-2019 at 16:49

12 percent is about what they use. Homemade can have more.