uniform corrosion

aeacfm - 11-12-2010 at 09:05


Does uniform corrosion is electrochemical (anodic & cathodic sites) or chemical corrosion (oxidation of metal)?:mad:

jokull - 11-12-2010 at 21:23

Uniform corrosion originates from chemical attack.

aeacfm - 12-12-2010 at 01:13

so you mean no anodic no cathodic sites found

psychokinetic - 12-12-2010 at 02:06

If it was uniform, wouldn't that exclude the possibility of different regions?

aeacfm - 12-12-2010 at 03:37

Quote: Originally posted by psychokinetic  
If it was uniform, wouldn't that exclude the possibility of different regions?

yea , thats what i understand but in a cprrosion course the instructor said that there is anodic and cathodic sites but we cant separate them , so by this way he exclude that it is chemical and mean that it is electrochemical ???