Describe your recrystallisation process in detail. Too often I've seen someone "crystallising" a product by boiling off all the solvent and frying
the solid. There's plenty of 17th and 18th century texts describing the purification of saltpeter, worth a bit of digging on the Internet Archives,
Google Books, and elsewhere. |