Sciencemadness Discussion Board

Beryllium powder 99% for sale

Chemcraft - 4-3-2020 at 08:38

We offer beryllium powder for sale. Packed in plastic jars.
Price for 50 gr - 195 USD
Worldwide shipping

Main substance: >99%
Density: 0.57 - 0.61 g/cm3
Average particle size: 14-19 µm
Maximum particle size: 30 µm
Specific surface area: 0.9-1.0 m2/g


Link to our internet store:
https://chemcraft.su/product/24324



Be powder -2.jpg - 805kB

Herr Haber - 4-3-2020 at 11:19

So sad you didnt have it 10 days ago !


Oh well, next time.

MineMan - 12-3-2020 at 01:27

I thought I read somewhere the CIA used beryllium for assassinations. It was an interesting read but I can’t find it now...

Is it really that toxic? A quick google search was useless.

B(a)P - 12-3-2020 at 02:08

ATSDR has some good info on this, mainly a risk from an inhalation exposure scenario.
https://www.atsdr.cdc.gov/ToxProfiles/tp4.pdf

The toxicity of beryllium to the respiratory tract is usually manifested in one of
two syndromes: acute beryllium disease and chronic beryllium disease. Acute beryllium disease is
usually observed at relatively high beryllium exposure levels, has a short period of induction, and is
usually resolved within a couple of months of exposure termination. It is believed to be an inflammatory
response to beryllium and most regions of the respiratory tract are affected; some reported symptoms
include nasopharyngitis, shortness of breath, labored breathing, and chemical pneumonitis.

Two types of dermal effects have been observed in beryllium exposed workers: an
inflammatory reaction and an immune reaction. Edematous papulovesicular dermatitis was observed in
workers exposed to airborne beryllium sulfate, beryllium fluoride, or beryllium oxyfluoride; this is likely
an inflammatory response to beryllium.