| I think most people have a shallow understanding of chemistry. I usually respond by explaining they use it every day as well, I just seek a deeper
understanding so I can take advantage of it and perhaps create something unique. Most of my hobby centers around plating and electroforming, pigments,
dyes, oxidizing patinas, etc., because I like to integrate it with art. Below is a raccoon skull I electroformed with copper. I have done similar
electroforms capturing stones and other objects with nickel as well. |