I used to have an evaporating dish from Pyrex that I broke.

Does anyone know of a sturdy glass bowl from Pyrex that I can use as a oil bath for 2000ml RBFs

I'm trying to avoid metal as I have a hotplate stirrer from corning.

I also don't want to be heating this and it shatter.

Any suggestions?

Dr.Bob - 10-2-2022 at 08:46

A 190 mm Pyrex Crystallizing dish is ideal for that purpose. You can find them used on Ebay.

Fery - 10-2-2022 at 10:44

I've bought few pieces of used kitchen aluminium pots of various sizes from second hand shop (1-2 EUR per piece).