| That is a serious amount of corrosion to occur from a small amount of acid. Looking at the last image (63kB 5955x459), it looks like a large amount of
brass has been removed from the lower half of the lock. It seems as though the stainless steel is somewhat immune, but the brass and chrome coated
steel has been heavily corroded. |