| I noticed plastic clamps breaking too during Cl2 experiments but I thought it was due to sulfuric acid grease. They must be really sensitive to
chlorine if it's that since I did a multi-day chlorination experiment (chloral prep) in my bedroom and it was fine to sleep in there. Only a mild
odor, no irritation or anything like that |